Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | -36.0 °C | -32.8 °F | Midpoint; ASTM E 1269 |
Huntsman IROGRAN® PS 455-204 TPU-Polyester Polyester-based grades with a broad processing window ideally suited for cast, flat die and flown film lines.Information provided by Alliance Polymers |
|||
Glass Transition Temp, Tg | -36.0 °C | -32.8 °F | |
Huntsman KRYSTALFLEX® PE 399 Polyurethane Optical Aliphatic Film Key Properties:Moisture ResistanceChemical CompatibilityCooler ProcessingHigher AdhesionMultiple Design OptionNo special storage requiredInformation provided by Alliance Polymers |
|||
Glass Transition Temp, Tg | -36.0 °C | -32.8 °F | |
Huntsman KRYSTALFLEX® PE 399 Polyurethane Optical Aliphatic Film Key Properties:Moisture ResistanceChemical CompatibilityCooler ProcessingHigher AdhesionMultiple Design OptionNo special storage requiredInformation provided by Alliance Polymers |
|||
Glass Transition Temp, Tg | -36.0 °C | -32.8 °F | HR 10 K/min, half height |
Styron Sprintan® SLR 6430 Solution Styrene Butadiene Rubber (S-SBR) Composition: SPRINTAN® SLR-6430 – Schkopau is manufactured by anionic solution polymerization using an organo-lithium initiator. In relation to solid rubber the grade is extended with 37.5 p.. |
|||
Glass Transition Temp, Tg | -36.0 °C | -32.8 °F | ASTM D3418 |
DuPont Elvaloy® 4924 Ethylene/Vinyl Acetate/Carbon Monoxide Copolymer Specialized copolymers deliver flexibility, toughness and weatherability to adhesives, plastics, highways and roofing.Availability: GloballyInformation provided by DuPont. |
|||
Glass Transition Temp, Tg | -36.0 °C | -32.8 °F | |
Zeon Chemicals Hydrin® T3100 Polyepichlorohydrin Elastomer Hydrin T3100 is an epichlorohydrin/ethylene oxide/allyl glycidyl ether terpolymer with high oil, fuel and solvent resistance. Compounds using Hydrin T3100 typically exhibit good heat resistance, exc.. |
|||
Glass Transition Temp, Tg | -36.0 °C | -32.8 °F | DSC |
Lubrizol ESTANE® ETE50DS3 Ester Based Thermoplastic Polyurethane Features: Excellent physical and low temperature properties with very good chemical resistance and wide processing window for extrusion.Uses: Flat die/cast film and tubing extrusion and Injection an.. |
|||
Glass Transition Temp, Tg | -36.0 °C | -32.8 °F | DSC |
Lubrizol ESTANE® ETE55DT3 Ester Based Thermoplastic Polyurethane Features: Hard TPU with wide extrusion processing window and melt stability, low temperature flexibility, high transparency, UV stableUses: Extrusion: Hose and Tube, Extrusion: Profile, Cable Jacket.. |
|||
Glass Transition Temp, Tg | -36.0 °C | -32.8 °F | DSC |
Lubrizol Estane® 2355-85ABR Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: FDA and USDA compliance, Blend resinAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by Lubrizol.Lubrizol acquired the Pellethane product l.. |
|||
Glass Transition Temp, Tg | -36.0 °C | -32.8 °F | 10°C/min |
Covestro Texin® 390 Urethane Thermoplastic Elastomer Key Features:UnfilledSuitable processing methods:Injection moldingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adop.. |
|||
Glass Transition Temp, Tg | -36.0 °C | -32.8 °F | 10°C/min |
Arkema Group Kynar® FLEX 2800 PVDF
(discontinued **) Designation ISO 12086-VDF/HFP-K, EG1N, N. ?E7.D.G.B.C,, ? (3.5-7.5)Kynar FLEX PVDF are fluorinated thermoplastic copolymers.Outstanding characteristics of Kynar FLEX: chemical resistance, impervious.. |
|||
Glass Transition Temp, Tg | -36.0 °C | -32.8 °F | 10°C/min |
Arkema Group Kynar® FLEX 2801 PVDF
(discontinued **) Designation ISO 12086-VDF/HFP-K, EDN, N. ?E7.D.G.B.C,, ? (3.5-7.5)Kynar FLEX PVDF are fluorinated thermoplastic copolymers.Outstanding characteristics of Kynar FLEX: chemical resistance, imperviousn.. |
|||
Glass Transition Temp, Tg | -36.0 °C | -32.8 °F | 10°C/min |
Arkema Group Kynar® FLEX 2821 PVDF
(discontinued **) Designation ISO 12086-VDF/HFP-K, EDN, N. ?E5.C.H.B.C,, ? (2.5-6.5)Kynar FLEX PVDF are fluorinated thermoplastic copolymers.Outstanding characteristics of Kynar FLEX: chemical resistance, imperviousn.. |
|||
Glass Transition Temp, Tg | -36.0 °C | -32.8 °F | 10°C/min |
Arkema Group Kynar® FLEX 2822 PVDF
(discontinued **) Designation ISO 12086-VDF/HFP-K, EDN, N. ?E5.C.H.B.C,, ? (4-8)Kynar FLEX PVDF are fluorinated thermoplastic copolymers.Outstanding characteristics of Kynar FLEX: chemical resistance, imperviousness .. |