Polymer Property : Glass Transition Temp, Tg = -27.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -27.0 °C
-16.6 °F
DMA
Covestro Texin® 5250 Thermoplastic Polyurethane, Polyether-based, Medical  (discontinued **)
This grade is in chemical compliance with 21 CFR 177.1680 (Polyurethane Resins) and 177.2600 (Rubber articles intended for repeated use) subject to the limitations of this regulation and any other r..
Glass Transition Temp, Tg -27.0 °C
-16.6 °F
Dow Pellethane® 2103-90AEF Polyurethane Elastomer, Ether Based  (discontinued **)
PELLETHANE® 2103-90AEF elastomer is a polytetramethylene glycol ether based polyurethane elastomer, featuring superior resilience, low temperature properties, excellent hydrolytic stability, and re..
Glass Transition Temp, Tg -27.0 - 225 °C
-16.6 - 437 °F
Average value: 100 °C Grade Count:82
Overview of materials for Epoxy Encapsulant, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Encapsulant, Unreinforced". Each property range of values reported is minimum and maximum values o..
Glass Transition Temp, Tg -27.0 °C
-16.6 °F
Mallard Creek Polymers Rovene® 4125 Styrene-Butadiene Emulsion
Applications: Rovene® 4125 is recommended for applications where a primer-sealer that provides adhesion between asphalt and other various surface treatments is needed. Rovene® 4125 has been us..
Glass Transition Temp, Tg -27.0 °C
-16.6 °F
Styron DL 221NA Carboxylated SB
Performance Features: Excellent water and heat resistanceApplications: Glass Fiber Binding and NonwovensLatin America/South AmericaInformation provided by Styron
Glass Transition Temp, Tg -27.0 °C
-16.6 °F
Loctite® 3143 Deep Potting Epoxy
PottersLoctite® Potting materials are used on electronic device housings to enhance mechanical strength, provide electrical insulation and enhance vibration and shock resistance of assemblies. For ..
Glass Transition Temp, Tg -27.0 °C
-16.6 °F
Loctite® 3166 Deep Potting Epoxy
PottersLoctite® Potting materials are used on electronic device housings to enhance mechanical strength, provide electrical insulation and enhance vibration and shock resistance of assemblies.For e..
Glass Transition Temp, Tg -27.0 °C
-16.6 °F
DSC
Lubrizol Estane® 2103-90AEFH Thermoplastic Polyurethane Elastomer
Formerly PellethaneFeature: Film resin for injection blow moldingAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by Lubrizol.Lubrizol acquired the Pellethane product ..
Glass Transition Temp, Tg -27.0 °C
-16.6 °F
DSC
Lubrizol Estane® 2103-90AEL Film Grade Thermoplastic Polyurethane Elastomer
Formerly PellethaneFeature: Film resin for injection blow moldingAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by Lubrizol.Lubrizol acquired the Pellethane product ..
Glass Transition Temp, Tg -27.0 °C
-16.6 °F
10°C/min
Covestro Texin® 950U Urethane Thermoplastic Elastomer
Key Features:UnfilledU.V. stabilized or stable to weatherSuitable processing methods:Injection moldingProfile extrusionSheet extrusionInformation provided by Bayer Polymers.As of 1 September 2015, B..
Glass Transition Temp, Tg -27.0 °C
-16.6 °F
DuPont Test Method
DuPont Performance Polymers Kalrez® Spectrum™ 0040 Fluoroelastomer
Kalrez® Spectrum™ 0040 perfluoroelastomer parts are specifically designed for low-temperature environments where significant chemical resistance is required. Proprietary polymer and cure technolog..
Glass Transition Temp, Tg -27.0 °C
-16.6 °F
ASTM D3418
DSM Biomedical PurSil® 20 Thermoplastic Silicone Polyether Polyurethane (TSPU)
A novel copolymer that is strong yet flexible with proven biocompatibility and biostability Combining the benefits of both silicone elastomers and polyether urethanes, PurSil® TSPU has exceptional..
Glass Transition Temp, Tg -27.0 °C
-16.6 °F
10°C/min
Covestro Texin® 950 Urethane Thermoplastic Elastomer
Key Features:UnfilledSuitable processing methods:Injection moldingProfile extrusionSheet extrusionInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScience was separated f..