Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | -8.00 - -2.00 °C | 17.6 - 28.4 °F | |
Metabolix Mirelâ„¢ I6001 Biobased Polymeric Modifier I6001 is an effective multifunctional, >85% biobased polymeric modifier for semi-rigid and flexible PVC compounds. It improves impact resistance, tear resistance, tensile toughness and plasticizatio.. |