Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | -15.0 - 1.00 °C | 5.00 - 33.8 °F | Metabolix STM-003 |
Metabolix Mirelâ„¢ I6003rp Biobased PHA Polymeric Modifier I6003rp PHA enhances the processing and properties of recycled PVC. Offering excellent inherent miscibility in PVC to enable improved processing, I6003rp can lower torque and improve flow, while imp.. |
|||
Glass Transition Temp, Tg | -15.0 °C | 5.00 °F | DSC |
Lubrizol ESTANE® 58137 Ester Based Thermoplastic Polyurethane Features: Fast cycling, broad temperature performance, and durabilityUse: Injection MoldingAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol. |
|||
Glass Transition Temp, Tg | -15.0 °C | 5.00 °F | DSC |
Lubrizol Estane® 2355-95AE Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Fuel resistant, extrusion laminate coatingAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by Dow Chemical.Lubrizol acquired the Pellethane.. |
|||
Glass Transition Temp, Tg | -15.0 °C | 5.00 °F | DSC |
Lubrizol Estane® 2355-95AEF Thermoplastic Polyurethane Type: Pellethane® 2355-95AEF is a thermoplastic polyurethane elastomer.Feature: Film resin, Fuel resistant, Blow molding grade resin.Information Provided by The Lubrizol Corporation |
|||
Glass Transition Temp, Tg | -15.0 °C | 5.00 °F | 10°C/min |
Covestro Texin® 260 Urethane Thermoplastic Elastomer Key Features:UnfilledSuitable processing methods:Injection moldingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adop.. |
|||
Glass Transition Temp, Tg | -15.0 °C | 5.00 °F | |
Dow Latex XZ 92227.01 Experimental Latex Description: XZ 92227.01 Experimental Latex is an aqueous dispersion of a modified carboxylated styrene butadiene copolymer. It has been developed for use as soft precoat and adhesive latex with sup.. |
|||
Glass Transition Temp, Tg | -15.0 °C | 5.00 °F | Inflection |
Dow Advanta® 3650 Specialty Elastomer
(discontinued **) Advanta® specialty elastomers provides good fluid resistance and better high temperature performance than nitrile or HNBR and lower cost than fluoroelastomers. Available in two grades. ASTM D2000.. |