Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 2.02 J/g-°C | 0.483 BTU/lb-°F | |
Styron CALIBRE™ 200 10 Polycarbonate, General Purpose CALIBRE® 200 series are general purpose, UL listed Polycarbonate resins formulated to comply with the applicable FDA and European regulations governing food contact(1). CALIBRE 200 series resins .. |