Thermal Properties Metric English Comments
Specific Heat Capacity 1.97 J/g-°C
0.470 BTU/lb-°F
Saint-Gobain Norton® PMP Film
Features/Benefits:Good release properties for up to 180°C (356°F) cure composites (application dependent)low density for high surface area per poundExcellent clarityThermoformableProduct avail..
Specific Heat Capacity 1.97 J/g-°C
0.471 BTU/lb-°F
ASTM C351
Mitsui TPX® DX820 Methylpentene Copolymer
TPX® is a 4-methylpentene-1 based polyolefin with a unique combination of transparency, heat and chemical resistant qualities. TPX is used in a wide variety of applications, including: medical equi..
Specific Heat Capacity 1.97 J/g-°C
0.471 BTU/lb-°F
ASTM C351
Mitsui TPX® MX002 Methylpentene Copolymer
TPX® is a 4-methylpentene-1 based polyolefin with a unique combination of transparency, heat and chemical resistant qualities. TPX is used in a wide variety of applications, including: medical equi..
Specific Heat Capacity 1.97 J/g-°C
0.471 BTU/lb-°F
ASTM C351
Mitsui TPX® MX004 Methylpentene Copolymer
TPX® is a 4-methylpentene-1 based polyolefin with a unique combination of transparency, heat and chemical resistant qualities. TPX is used in a wide variety of applications, including: medical equi..
Specific Heat Capacity 1.97 J/g-°C
0.471 BTU/lb-°F
ASTM C351
Mitsui TPX® RT18 Methylpentene Copolymer, Transparent Grade
TPX® is a 4-methylpentene-1 based polyolefin with a unique combination of transparency, heat and chemical resistant qualities. TPX is used in a wide variety of applications, including: medical equi..
Specific Heat Capacity 1.97 J/g-°C
0.471 BTU/lb-°F
ASTM C351
Mitsui TPX® RT18 XB Methylpentene Copolymer
TPX® is a 4-methylpentene-1 based polyolefin with a unique combination of transparency, heat and chemical resistant qualities. TPX is used in a wide variety of applications, including: medical equi..