Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.60 J/g-°C @Temperature 100 °C |
0.382 BTU/lb-°F @Temperature 212 °F |
ASTM E1269 |
Eastman 9921P PET Injection Molded
(discontinued **) Voridian PET 9921P is produced at Voridian’s manufacturing sites in Rotterdam and Zarate, it is PTA/CHDM based, and it is sold to customers in the Europe, Middle East and Africa, Argentina, Bolivia.. |
|||
Specific Heat Capacity | 1.60 J/g-°C @Temperature 100 °C |
0.382 BTU/lb-°F @Temperature 212 °F |
|
Solvay Specialty Polymers Solef® 21508 PVDF Copolymer
(discontinued **) Key features of this grade: High Elongation, Wire & Cable, Plenum, Formulated. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® P.. |
|||
Specific Heat Capacity | 1.60 J/g-°C @Temperature 100 °C |
0.382 BTU/lb-°F @Temperature 212 °F |
|
Solvay Specialty Polymers Solef® 31008 PVDF Copolymer
(discontinued **) Key features of this grade: High Flexibility/ High Elongation/Cold Impact Resistance, Wire & Cable, Plenum, Formulated. Recommended processing is extrusion. Available as powder & granules.General .. |
|||
Specific Heat Capacity | 1.60 J/g-°C @Temperature 100 °C |
0.382 BTU/lb-°F @Temperature 212 °F |
|
Solvay Specialty Polymers Solef® 1015/0078 PVDF Homopolymer
(discontinued **) Key features of this grade: Plasticized, Offshore, Piping, Formulated. Recommended processing is extrusion. Available as granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorina.. |
|||
Specific Heat Capacity | 1.60 J/g-°C @Temperature 100 °C |
0.382 BTU/lb-°F @Temperature 212 °F |
ASTM C351 |
Solvay Specialty Polymers Ajedium™ PVDF 9009 Polyvinylidene Fluoride (PVDF) Solef® 9009 PVDF homopolymer is a semi-crystalline fluoropolymer. Solef® film is chemically inert to most acids, aliphatic and aromatic organic compounds, chlorinated solvents and alcohols.Fea.. |
|||
Specific Heat Capacity | 1.60 J/g-°C | 0.382 BTU/lb-°F | DSC |
Eastman Eastobond 19411 Copolyester, Film Eastobond 19411 is a terephthalate-based copolyester which is amorphous. It offers excellent organoleptic and gas-barrier properties. Eastobond 19411 has low postextrusion crystallinity and a low so.. |
|||
Specific Heat Capacity | 1.60 J/g-°C | 0.382 BTU/lb-°F | DSC |
Eastman Eastobond 19412 Copolyester, Film Eastobond 19412 is a terephthalate-based copolyester. It is identical to our 19411 resin in every aspect, except that the 19412 has been crystallized for drying purposes and ease of handling. Eastob.. |
|||
Specific Heat Capacity | 1.60 J/g-°C | 0.382 BTU/lb-°F | DSC |
Eastman Neostar FN005 Elastomer Neostar FN005 elastomer is a tough, clear, durable copolyester ether. It was designed for use in the profile and automotive markets, but is also used in packaging and tubing applications where tough.. |
|||
Specific Heat Capacity | 1.60 J/g-°C | 0.382 BTU/lb-°F | Melt |
Covestro Makrolon® 9415 Polycarbonate, 10% Glass Filled ISO 7391-PC,MFR,(,,)-09-9,GF10Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 min10 % Glass fiber reinforcedChlorine- and bromine-free flame retardantUL 94V-0/1.5 mm and 5VA/3.0 mmHigh viscosityEasy rel.. |
|||
Specific Heat Capacity | 1.60 J/g-°C | 0.382 BTU/lb-°F | Melt |
Covestro Makrolon® 9417 Polycarbonate, 10% Glass Filled ISO 7391-PC,MFLR,(,,)-09-9,GF10Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 min10 % Glass fiber reinforcedChlorine- and bromine-free flame retardantUL 94V-0/1.5 mm and 5VA/3.0 mmHigh viscosityUV stab.. |
|||
Specific Heat Capacity | 1.60 J/g-°C | 0.382 BTU/lb-°F | Melt |
Covestro Makrolon® DP1-1887* Polycarbonate, 10% Glass Filled ISO 7391-PC,MR,(,,)-18-9,GF10Developmental productMVR (300 °C/1.2 kg) 16 cm3/10 min10 % Glass fiber reinforcedMilled fiberLow viscosityEasy releasegood surface qualityInjection molding - Melt tempe.. |
|||
Specific Heat Capacity | 1.60 J/g-°C | 0.382 BTU/lb-°F | IEC 1006 |
BASF Ultradur B 4040 G10 BK5110 50% Glass Filled PBT Injection-molding grades containing 50% of glass fibers, for industrial parts with excellent surface quality.Applications: External door handles in vehicles, visible sunroof frames, over door handle.. |
|||
Specific Heat Capacity | 1.60 J/g-°C | 0.382 BTU/lb-°F | |
BASF Ultramid® A3WG5 25% Glass Filled PA66 (Conditioned) Ultramid A3WG5 is a 25% glass fiber reinforced and heat resistance injection molding PA66 grade. |
|||
Specific Heat Capacity | 1.60 J/g-°C | 0.382 BTU/lb-°F | |
BASF Ultramid® B35EG3 15% Glass Filled PA6 (Conditioned) Description: 15% glass-fiber reinforced injection-molding grade for gIT applications such as, for example, steering column switches, vehicle mirror housings and the wheels of mountain bikes.Informat.. |
|||
Specific Heat Capacity | 1.60 J/g-°C | 0.382 BTU/lb-°F | |
BASF Ultramid® B35EG3 15% Glass Filled PA6 (Dry) Description: 15% glass-fiber reinforced injection-molding grade for gIT applications such as, for example, steering column switches, vehicle mirror housings and the wheels of mountain bikes.Informat.. |
|||
Specific Heat Capacity | 1.60 J/g-°C | 0.382 BTU/lb-°F | |
BASF Ultramid® B3EG3 15% Glass Filled PA6 (Conditioned) Description: 15% glass-fiber reinforced injection-molding grade with enhanced impact resistance, for example, for vehicle mirror housings as well as for the wheels of mountain bikes.Information prov.. |
|||
Specific Heat Capacity | 1.60 J/g-°C | 0.382 BTU/lb-°F | |
BASF Ultramid® B3EG3 15% Glass Filled PA6 (Dry) Description: 15% glass-fiber reinforced injection-molding grade with enhanced impact resistance, for example, for vehicle mirror housings as well as for the wheels of mountain bikes.Information prov.. |
|||
Specific Heat Capacity | 1.60 J/g-°C @Temperature 100 °C |
0.382 BTU/lb-°F @Temperature 212 °F |
|
Solvay Specialty Polymers Solef® 1008 PVDF Homopolymer
(discontinued **) Key features of this grade: Low Viscosity, All Purpose, Injection, Virgin. Recommended processing is injection. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVDF .. |
|||
Specific Heat Capacity | 1.60 J/g-°C @Temperature 100 °C |
0.382 BTU/lb-°F @Temperature 212 °F |
|
Solvay Specialty Polymers Solef® 1009 PVDF Homopolymer
(discontinued **) Key features of this grade: Mean Viscosity, All Purpose, Injection/Extrusion, Virgin. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SO.. |
|||
Specific Heat Capacity | 1.60 J/g-°C @Temperature 100 °C |
0.382 BTU/lb-°F @Temperature 212 °F |
|
Solvay Specialty Polymers Solef® 1012 PVDF Homopolymer
(discontinued **) Key features of this grade: High Viscosity, Virgin. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinated semi-c.. |
|||
Specific Heat Capacity | 1.60 J/g-°C @Temperature 100 °C |
0.382 BTU/lb-°F @Temperature 212 °F |
|
Solvay Specialty Polymers Solef® 11008 PVDF Copolymer
(discontinued **) Key features of this grade: Low Viscosity, Wire & Cable, Plenum, Formulated. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVD.. |
|||
Specific Heat Capacity | 1.60 J/g-°C @Temperature 100 °C |
0.382 BTU/lb-°F @Temperature 212 °F |
|
Solvay Specialty Polymers Solef® 20810 PVDF Copolymer
(discontinued **) Key features of this grade: Li Battery, Virgin. Recommended processing is solution. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinated semi-crysta.. |