Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.05 J/g-°C | 0.250 BTU/lb-°F | ASTM E1461 |
Park Electrochemical Nelco® N7000-2 HT/N7000-3 Toughened Polyimide Laminate and Prepreg The Nelco N7000-2 HT laminate and N7000-3 prepreg are a series of toughened polyimide materials for use in high-reliability multilayers. This combined resin system provides excellent thermal perform.. |
|||
Specific Heat Capacity | 1.05 J/g-°C | 0.251 BTU/lb-°F | |
Zircar Zirconia M-45 Alumina Boards, Discs & Cylinders Insulation Zircar alumina insulation Type M Buster is a rigid, fibrous ceramic material produced by vacuum forming alumina fibers with with silica binders in BusterM that form a thermal shock resistant mullite.. |
|||
Specific Heat Capacity | 1.05 J/g-°C @Temperature 400 °C |
0.251 BTU/lb-°F @Temperature 752 °F |
|
Unifrax Excelfrax® 1900 Panel Microporous Insulation Unifrax Corporation's Excelfrax® product line, based on advanced microporous insulation technology, is a family of products which all exhibit superior insulating characteristics. Excelfrax micropo.. |
|||
Specific Heat Capacity | 1.05 J/g-°C | 0.251 BTU/lb-°F | DSC |
Wolf Kunststoff ZEDEX® ZX-324V2T A3F PEEK, PTFE Modified Reduced friction; High wear resistance; High elasticity; Stress resistantApplications: Shipbuilding; Chemical Engineering; Automotive Technology; Machine ToolsInformation provided by Zedex |
|||
Specific Heat Capacity | 1.05 J/g-°C | 0.250 BTU/lb-°F | |
Zircar Ceramics AL-30AAH Alumina Insulation AL-30AAH was developed for use in copper vapor lasers where the ultimate in low mass alumina purity is required.Information provided by Zircar Ceramics. |
|||
Specific Heat Capacity | 1.05 J/g-°C | 0.250 BTU/lb-°F | |
Zircar Ceramics ALBF Alumina Bulk Fiber Alumina Bulk Fiber Type ALBF consists of long aluminum oxide fibers suited for the vacuum forming of low density shapes. The high alpha alumina content and addition of a grain growth inhibitor give .. |
|||
Specific Heat Capacity | 1.05 J/g-°C | 0.250 BTU/lb-°F | |
Zircar Ceramics ALBF-1 Alumina Bulk Fiber Type ALBF-1 Alumina Bulk Fiber is a specially cleaned alumina fiber with relatively short fiber lengths. It is suitable for use in vacuum forming of high density rigid boards & shapes, in the reinfo.. |
|||
Specific Heat Capacity | 1.05 J/g-°C | 0.250 BTU/lb-°F | |
Zircar Ceramics ALC Alumina Insulation ALC is the same material as ZAL-15 - but brings exceptional uniformity in an insulation material in cylindrical form.Information provided by Zircar Ceramics. |
|||
Specific Heat Capacity | 1.05 J/g-°C | 0.250 BTU/lb-°F | |
Zircar Ceramics ECO-20AA Alumina Insulation ECO-20AA is most commonly utilized as hotface insulation in furnaces with hydrogen rich atmospheres such as bright annealing furnaces.Information provided by Zircar Ceramics. |
|||
Specific Heat Capacity | 1.05 J/g-°C | 0.250 BTU/lb-°F | |
Zircar Ceramics SALI Alumina Insulation SALI has been serving 1700°C low mass furnace users longer than any other alumina fiber board available today. SALI is a premium grade rigid fiber board with superior hot strength.Information provi.. |
|||
Specific Heat Capacity | 1.05 J/g-°C | 0.250 BTU/lb-°F | |
Zircar Ceramics ZAL-15AA Alumina Insulation ZAL-15 is a low thermal conductivity uniformly bound fiber board. It is ideal for machining into precision thermal insulators.Information provided by Zircar Ceramics. |
|||
Specific Heat Capacity | 1.05 J/g-°C | 0.250 BTU/lb-°F | |
Zircar Zirconia Buster A-30 Alumina Board, Disc, and Cylinder Insulation Zircar alumina insulation Type Buster is a rigid, fibrous ceramic material produced by vacuum forming alumina fibers with either a high purity alumina binder in BusterA-30 for use at 1600C or with s.. |
|||
Specific Heat Capacity | 1.05 J/g-°C | 0.250 BTU/lb-°F | |
Zircar Zirconia Buster M-15 Alumina Boards, Discs & Cylinders Insulation Zircar alumina insulation Type M Buster is a rigid, fibrous ceramic material produced by vacuum forming alumina fibers with with silica binders in BusterM that form a thermal shock resistant mullite.. |
|||
Specific Heat Capacity | 1.05 J/g-°C | 0.250 BTU/lb-°F | |
Zircar Ceramics ZAL-45 Alumina Insulation ZAL-45 is an exceptionally strong low density alumina fiber product. Alumina bonded ZAL-45AA is useful in reducing conditions.Information provided by Zircar Ceramics. |
|||
Specific Heat Capacity | 1.05 J/g-°C | 0.251 BTU/lb-°F | DuPont 990 test |
DuPont™ Tedlar® TWH20BS3 Satin White Polyvinyl Fluoride Film Properties of DuPont™ Tedlar® polyvinyl fluoride (PVF) biaxially oriented film include excellent resistance to weathering, outstanding mechanical properties, and inertness towards a wide variety o.. |
|||
Specific Heat Capacity | 1.05 J/g-°C @Temperature 500 °C |
0.251 BTU/lb-°F @Temperature 932 °F |
|
3M Nextel™ AF-10 Aerospace Woven Fabric 312 Information provided by 3M |
|||
Specific Heat Capacity | 1.05 J/g-°C @Temperature 500 °C |
0.251 BTU/lb-°F @Temperature 932 °F |
|
3M Nextel™ AF-10 Industrial Woven Fabric 312 Information provided by 3M |
|||
Specific Heat Capacity | 1.05 J/g-°C @Temperature 500 °C |
0.251 BTU/lb-°F @Temperature 932 °F |
|
3M Nextel™ AF-10 w/o sizing Aerospace Woven Fabric 312 Information provided by 3M |
|||
Specific Heat Capacity | 1.05 J/g-°C @Temperature 500 °C |
0.251 BTU/lb-°F @Temperature 932 °F |
|
3M Nextel™ AF-11 Aerospace Woven Fabric 312 Information provided by 3M |
|||
Specific Heat Capacity | 1.05 J/g-°C @Temperature 500 °C |
0.251 BTU/lb-°F @Temperature 932 °F |
|
3M Nextel™ AF-11 Industrial Woven Fabric 312 Information provided by 3M |
|||
Specific Heat Capacity | 1.05 J/g-°C @Temperature 500 °C |
0.251 BTU/lb-°F @Temperature 932 °F |
|
3M Nextel™ AF-11 w/o sizing Aerospace Woven Fabric 312 Information provided by 3M |
|||
Specific Heat Capacity | 1.05 J/g-°C @Temperature 500 °C |
0.251 BTU/lb-°F @Temperature 932 °F |
|
3M Nextel™ AF-12 Industrial Woven Fabric 312 Information provided by 3M |
|||
Specific Heat Capacity | 1.05 J/g-°C @Temperature 500 °C |
0.251 BTU/lb-°F @Temperature 932 °F |
|
3M Nextel™ AF-12 w/o sizing Aerospace Woven Fabric 312 Information provided by 3M |
|||
Specific Heat Capacity | 1.05 J/g-°C @Temperature 500 °C |
0.251 BTU/lb-°F @Temperature 932 °F |
|
3M Nextel™ AF-20 Industrial Woven Fabric 312 Information provided by 3M |
|||
Specific Heat Capacity | 1.05 J/g-°C @Temperature 500 °C |
0.251 BTU/lb-°F @Temperature 932 °F |
|
3M Nextel™ AF-30 Industrial Woven Fabric 312 Information provided by 3M |
|||
Specific Heat Capacity | 1.05 J/g-°C @Temperature 500 °C |
0.251 BTU/lb-°F @Temperature 932 °F |
|
3M Nextel™ AF-40 Industrial Woven Fabric 312 Information provided by 3M |
|||
Specific Heat Capacity | 1.05 J/g-°C | 0.250 BTU/lb-°F | |
Parkway Products Thixomolded® AZ91D Magnesium Thixomolding® is a fabrication technique, similar to injection molding, that uses magnesium alloys as the “resin” instead of plastic. Solid magnesium alloy pellets are fed into the machine, heate.. |
|||
Specific Heat Capacity | 1.05 J/g-°C | 0.250 BTU/lb-°F | |
Zircar Ceramics ZAL-45AA Alumina Insulation ZAL-45 is an exceptionally strong low density alumina fiber product. Alumina bonded ZAL-45AA is useful in reducing conditions.Information provided by Zircar Ceramics. |