Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.94 - 2.00 J/g-°C | 0.464 - 0.478 BTU/lb-°F | Average value: 1.99 J/g-°C Grade Count:6 |
Overview of materials for Nylon 6, 40% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Mineral Filled". Each property range of values reported is minimum and maximum values of ap.. |
|||
Specific Heat Capacity | 1.94 J/g-°C | 0.464 BTU/lb-°F | Melt |
Ineos ABS Triax® 1315 GF ABS + Polyamide Blend (Conditioned) Key Features:Contains FillerSuitable processing methods:Injection molding |
|||
Specific Heat Capacity | 1.94 J/g-°C | 0.464 BTU/lb-°F | Melt |