Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.92 J/g-°C | 0.459 BTU/lb-°F | ASTM C351 |
Solvay Specialty Polymers Polidan® T/A-HF Polyethylene, Crosslinked (XLPE) POLIDAN® T/A-HF is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for flexible crosslinkable pipes.Featu.. |