Thermal Properties Metric English Comments
Specific Heat Capacity 1.82 J/g-°C
0.435 BTU/lb-°F
Styron Pulse® B250 ABS + Polycarbonate
PULSE® B250 Engineering resin has been designed to provide a customized balance of low coefficient of linear thermal expansion, low temperature toughness and Class A surface finish paintability. ..
Specific Heat Capacity 1.82 J/g-°C
0.435 BTU/lb-°F
Melt
Covestro Makroblend® DP UT3907 Polycarbonate + PBT, Impact Grade
Developmental product(PC+PBT)-blendhigh flowimpact modifiedeasy releaseUV-stabilizedinjection molding grade Makroblend DP UT3907* offers superior flowability, good impact strength and excellent ch..
Specific Heat Capacity 1.82 J/g-°C
0.435 BTU/lb-°F
Melt
Covestro Makroblend® DP UT5005 Polycarbonate + PBT, Impact Grade
Developmental product(PC+PBT)-blendimpact modifiedeasy releaseinjection molding gradeMakroblend DP UT5005* provides an outstanding balance of low-temperature impact strength and flowability beside e..
Specific Heat Capacity 1.82 J/g-°C
0.435 BTU/lb-°F
Melt
Covestro Makroblend® DP UT5007 Polycarbonate + PBT, Impact Grade
Developmental product(PC+PBT)-blendimpact modifiedeasy releaseUV-stabilizedinjection molding grade Makroblend DP UT5007* provides an outstanding balance of low-temperature impact strength and flow..
Specific Heat Capacity 1.82 J/g-°C
0.435 BTU/lb-°F
Melt
Covestro Makroblend® DP UT6000 Polycarbonate + PBT, Impact Grade
Developmental product(PC+PBT)-blendimpact modifiedinjection molding grade Makroblend DP UT6000* offers an exceptional low-temperature impact strength, good flowability and excellent chemical resis..
Specific Heat Capacity 1.82 J/g-°C
0.435 BTU/lb-°F
Melt
Covestro Makroblend® DP UT6003 Polycarbonate + PBT, Impact Grade
Developmental product(PC+PBT)-blendimpact modifiedUV-stabilizedinjection molding grade Makroblend DP UT6003* offers an exceptional low-temperature impact strength, good flowability and excellent c..
Specific Heat Capacity 1.82 J/g-°C
0.435 BTU/lb-°F
Melt
Covestro Makroblend® DP UT6005 Polycarbonate + PBT, Impact Grade
Developmental product(PC+PBT)-blendimpact modifiedeasy releaseinjection molding grade Makroblend DP UT6005* offers an exceptional low-temperature impact strength, good flowability and excellent ch..
Specific Heat Capacity 1.82 J/g-°C
0.435 BTU/lb-°F
Melt
Covestro Makroblend® KU 2-7915 Polycarbonate + PBT, Impact Grade
ISO 7792-1-PC/PBT,MHPR,-020(PC+PBT)-blendsimpact modifiedInjection molding gradeexcellent toughness at low temperaturesideal for painted applicationsunreinforcedPreprocessingMax. Water content
Specific Heat Capacity 1.82 J/g-°C
0.435 BTU/lb-°F
Melt
Covestro Makroblend® DP UT3905 Polycarbonate + PBT, Impact Grade
Developmental product(PC+PBT)-blendhigh flowimpact modifiedeasy releaseinjection molding grade Makroblend DP UT3905* offers superior flowability, good impact strength and excellent chemical resist..
Specific Heat Capacity 1.82 J/g-°C
0.435 BTU/lb-°F
Melt
Covestro Makroblend® KU 2-7912 Polycarbonate + PBT, Impact Grade
ISO 7792-1-PC/PBT,MHPR,-020(PC+PBT)-blendsimpact modifiedInjection molding grademedium flowhigh toughness at low temperaturesideal for painted applicationunreinforcedPreprocessingMax. Water content
Specific Heat Capacity 1.82 J/g-°C
0.435 BTU/lb-°F
Melt
Covestro Makroblend® KU 2-7912/4 Polycarbonate + PBT, Impact Grade
ISO 7792-1-PBT/PC,MHPR,-020(PC+PBT)-blendsimpact modifiedInjection molding gradehigh toughness at low temperaturesideal for painted applicationsunreinforcedPreprocessingMax. Water content
Specific Heat Capacity 1.82 J/g-°C
0.435 BTU/lb-°F
Melt
Covestro Makroblend® DP 6015 Polycarbonate + PBT
Developmental product(PC+PBT)-blendimpact modifiedeasy releaseinjection molding grade. Makroblend DP 6015* provides an outstanding balance of low-temperature impact strength and excellent chemical ..
Specific Heat Capacity 1.82 J/g-°C
0.435 BTU/lb-°F
Melt
Covestro Makroblend® DP UT6007 Polycarbonate + PBT, Impact Grade
Developmental product(PC+PBT)-blendimpact modifiedeasy releaseUV-stabilizedinjection molding grade Makroblend DP UT6007* offers an exceptional low-temperature impact strength, good flowability and..