Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.40 - 1.60 J/g-°C | 0.335 - 0.382 BTU/lb-°F | Average value: 1.49 J/g-°C Grade Count:3 |
Overview of materials for Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled". Specific grades with glass content between 45.. |
|||
Specific Heat Capacity | 1.60 - 1.60 J/g-°C @Temperature 100 - 100 °C |
0.382 - 0.382 BTU/lb-°F @Temperature 212 - 212 °F |
Average value: 1.60 J/g-°C Grade Count:21 |
Overview of materials for Polyvinylidinefluoride (PVDF), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polyvinylidinefluoride (PVDF), Molded/Extruded". Each property range of values reported is minimum and m.. |
|||
Specific Heat Capacity | 1.50 - 1.60 J/g-°C | 0.359 - 0.382 BTU/lb-°F | Average value: 1.58 J/g-°C Grade Count:6 |
Overview of materials for Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled". Each property range of values reported is mini.. |
|||
Specific Heat Capacity | 1.50 - 1.60 J/g-°C | 0.359 - 0.382 BTU/lb-°F | DSC |
Wacker Silicones Geniomer® 140 Silicone TPE SLM TPSE 140 is a silicone copolymer containing over 90% siloxane. Geniomer® is a two phase block copolymer made up of a soft polydimethylsiloxane (PDSM) phase and a hard aliphatic isocyanate phas.. |
|||
Specific Heat Capacity | 1.50 - 1.60 J/g-°C | 0.359 - 0.382 BTU/lb-°F | DSC |
Wacker Silicones Geniomer® 200 Silicone TPE Elastomer SLM TPSE 200 is a silicone copolymer containing over 90% siloxane. Geniomer® is a two phase block copolymer made up of a soft polydimethylsiloxane (PDSM) phase and a hard aliphatic isocyanate phas.. |
|||
Specific Heat Capacity | 1.50 - 1.60 J/g-°C | 0.359 - 0.382 BTU/lb-°F | DSC |
Wacker Silicones Geniomer® 80 Silicone TPE SLM TPSE 80 is a silicone copolymer containing over 90% siloxane. Geniomer® is a two phase block copolymer made up of a soft polydimethylsiloxane (PDSM) phase and a hard aliphatic isocyanate phase.. |
|||
Specific Heat Capacity | 1.50 - 1.60 J/g-°C | 0.359 - 0.382 BTU/lb-°F | DSC |
Wacker Silicones Geniomer® 60 Silicone TPE SLM TPSE 60 is a silicone copolymer containing over 90% siloxane. Geniomer® is a two phase block copolymer made up of a soft polydimethylsiloxane (PDSM) phase and a hard aliphatic isocyanate phase.. |