Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.573 J/g-°C | 0.3760 BTU/lb-°F | Melt |
BASF Petra® 140 45% Glass Filled PET Petra 140 is a 45% glass reinforced injection molding polyethylene terephthalate (PET) offering an increased level of strength, stiffness, high temperature performance and dimensional stability. Ex.. |