Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.423 J/g-°C @Temperature 300 °C |
0.3400 BTU/lb-°F @Temperature 572 °F |
DSC |
Mitsui AURUM® PL450C Polyimide