Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.25 J/g-°C | 0.299 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® 101R PC (Asia Pacific) Nonhalogenated. 7.0 MFR, for thicker sections without sinks. Internal mold release. |
|||
Specific Heat Capacity | 1.25 J/g-°C | 0.299 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® 121R PC (Asia Pacific) Nonhalogenated. 17.5 MFR, for small, intricate parts. Internal mold release. |
|||
Specific Heat Capacity | 1.25 J/g-°C | 0.299 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® 123R PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated. 17.5 MFR, for small, intricate parts. UV stabilized. Internal mold release. |
|||
Specific Heat Capacity | 1.25 J/g-°C | 0.299 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® 124 PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. 17.5 MFR, for small, intricate parts. FDA food contact compliant in limited colors.Effective January 15th, 2007 this grade.. |
|||
Specific Heat Capacity | 1.25 J/g-°C | 0.299 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® 131 PC Nonhalogenated. 3.5 MFR. |
|||
Specific Heat Capacity | 1.25 J/g-°C | 0.299 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® 141R PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated. 10.5 MFR. Internal mold release. |
|||
Specific Heat Capacity | 1.25 J/g-°C | 0.299 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® 144 PC UL rated HB. 200 series recommended when V-2 rating required. 10.5 MFR. FDA food contact compliant in limited colors.Effective January 15th, 2007 this grade will no longer be supported with bioco.. |
|||
Specific Heat Capacity | 1.25 J/g-°C | 0.299 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® 153R PC (Asia Pacific) Nonhalogenated. 2.5 MFR. Blowmolding/extrusion. UV-stabilized. Internal mold release. |
|||
Specific Heat Capacity | 1.25 J/g-°C | 0.299 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® 201R PC 7.0 MFR, for thicker sections without sinks. Improved flame retardance. Internal mold release. |
|||
Specific Heat Capacity | 1.25 J/g-°C | 0.299 BTU/lb-°F | ASTM C 351 |
SABIC Innovative Plastics Lexan® 221 PC 17.5 MFR, for small, intricate parts. Improved flame retardance.This data was supplied by SABIC-IP for the Americas region. |
|||
Specific Heat Capacity | 1.25 J/g-°C | 0.299 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® 221R PC (Asia Pacific) 17.5 MFR, for small, intricate parts. Improved flame retardance. Internal mold release. |
|||
Specific Heat Capacity | 1.25 J/g-°C | 0.299 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® 4504 PPC (Asia Pacific) High heat resistant polycarbonate copolymer, provides DTUL of 290F at 264 psi. FDA food contact compliant in limited colors. Effective January 15th, 2008 this grade will no longer be supported wit.. |
|||
Specific Heat Capacity | 1.25 J/g-°C | 0.299 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® FXE154 PC FDA compliant (color limited) PC. 2.5 MFR. Potable water/extrusion blowmoldable. ILLUMINATE special effects (fluorescent/edge glow colors). |
|||
Specific Heat Capacity | 1.25 J/g-°C | 0.299 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® HF1140R PC High flow grade. Heat stabilized. Enhanced level of mold release. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade will no longer be supported with biocompatib.. |
|||
Specific Heat Capacity | 1.25 J/g-°C | 0.299 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® HP1 PC (Asia Pacific) High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO sterilizable. Contains mold release. |
|||
Specific Heat Capacity | 1.25 J/g-°C | 0.299 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® HP4R PC Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). ETO and steam sterilizable. Contains a h.. |
|||
Specific Heat Capacity | 1.25 J/g-°C | 0.299 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® HPS1S PC High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, e-beam and gamma sterilizable. Contains.. |
|||
Specific Heat Capacity | 1.25 J/g-°C | 0.299 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® IFX5420Z PC (Asia Pacific) Lexan* IFX5420Z is a medium viscosity, release containing, injection moldable polycarbonate grade suitable for use in industry protective eye-ware welding applications. This grade meets the transmis.. |
|||
Specific Heat Capacity | 1.25 J/g-°C | 0.299 BTU/lb-°F | ASTM C 351 |
SABIC Innovative Plastics Lexan® ML7678 PC 17.5 MFR, for small, intricate parts. FDA food contact compliant in limited colors. Enhanced mold release package.This data was supplied by SABIC-IP for the Americas region. |
|||
Specific Heat Capacity | 1.25 J/g-°C | 0.299 BTU/lb-°F | ASTM C 351 |
SABIC Innovative Plastics Lexan® PPC4701 PPC High heat resistant polyphthlate carbonate, provides DTUL of 300F at 264 psi.This data was supplied by SABIC-IP for the Americas region. |
|||
Specific Heat Capacity | 1.25 J/g-°C | 0.299 BTU/lb-°F | ASTM C 351 |
SABIC Innovative Plastics Lexan® 134 PC (Asia Pacific) 3.5 MFR. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade is no longer supported with biocompatibility information and should not be used for medical applicati.. |
|||
Specific Heat Capacity | 1.25 J/g-°C | 0.299 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® 143 PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated. 10.5 MFR. UV-stabilized. |
|||
Specific Heat Capacity | 1.25 J/g-°C | 0.299 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® 143R PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated. 10.5 MFR. UV-stabilized. Internal mold release. |
|||
Specific Heat Capacity | 1.25 J/g-°C | 0.299 BTU/lb-°F | ASTM C 351 |
SABIC Innovative Plastics Lexan® 151 PC (Asia Pacific) Nonhalogenated. 2.5 MFR. Blowmolding/extrusion.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Specific Heat Capacity | 1.25 J/g-°C | 0.299 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® 4501 PPC High heat resistant polyphthlate carbonate, provides DTUL of 290F at 264 psi. |
|||
Specific Heat Capacity | 1.25 J/g-°C | 0.299 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® HP1R PC High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO sterilizable. Contains a higher amount.. |
|||
Specific Heat Capacity | 1.25 J/g-°C | 0.299 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® HP2NR PC Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no.. |
|||
Specific Heat Capacity | 1.25 J/g-°C | 0.299 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® HP6 PC Low/med flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains mo.. |
|||
Specific Heat Capacity | 1.25 J/g-°C | 0.299 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® HP6NR PC (Asia Pacific) Low/med flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no .. |
|||
Specific Heat Capacity | 1.25 J/g-°C | 0.299 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® HPH4704 PPC (Europe-Africa-Middle East) High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, gamma and e-beam steril.. |