Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Specific Heat Capacity = 0.289 BTU/lb-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Specific Heat Capacity 1.21 J/g-°C
0.289 BTU/lb-°F
ASTM C351
SABIC Innovative Plastics Lexan® 500 PC
10% GR PC. Optimum combination of high modulus plus excellent impact strength and flame retardance.
Specific Heat Capacity 1.21 J/g-°C
0.289 BTU/lb-°F
ASTM C351
SABIC Innovative Plastics Lexan® 500 PC (Asia Pacific)
10% GR PC. Optimum combination of high modulus plus excellent impact strength and flame retardance.
Specific Heat Capacity 1.21 J/g-°C
0.289 BTU/lb-°F
ASTM C351
SABIC Innovative Plastics Lexan® 500R PC
10% GR PC. Optimum combination of high modulus plus excellent impact strength and flame retardance. Internal mold release.
Specific Heat Capacity 1.21 J/g-°C
0.289 BTU/lb-°F
ASTM C351
SABIC Innovative Plastics Lexan® 500R PC (Asia Pacific)
10% GR PC. Optimum combination of high modulus plus excellent impact strength and flame retardance. Internal mold release.
Specific Heat Capacity 1.21 J/g-°C
0.289 BTU/lb-°F
ASTM C351
SABIC Innovative Plastics Lexan® 503 PC
10% GR PC. Optimum combination of high modulus plus excellent impact strength and flame retardance. UV-stabilized.
Specific Heat Capacity 1.21 J/g-°C
0.289 BTU/lb-°F
ASTM C351
SABIC Innovative Plastics Lexan® 503 PC (Asia Pacific)
10% GR PC. Optimum combination of high modulus plus excellent impact strength and flame retardance. UV-stabilized.
Specific Heat Capacity 1.21 J/g-°C
0.289 BTU/lb-°F
ASTM C351
SABIC Innovative Plastics Lexan® 503R PC
10% GR PC. Optimum combination of high modulus plus excellent impact strength and flame retardance. UV-stabilized. Internal mold release.
Specific Heat Capacity 1.21 J/g-°C
0.289 BTU/lb-°F
ASTM C351
SABIC Innovative Plastics Lexan® 503R PC (Asia Pacific)
10% GR PC. Optimum combination of high modulus plus excellent impact strength and flame retardance. UV-stabilized. Internal mold release.
Specific Heat Capacity 1.21 - 1.81 J/g-°C
0.289 - 0.433 BTU/lb-°F
Average value: 1.40 J/g-°C Grade Count:6
Overview of materials for Acetal Copolymer, 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% ar..
Specific Heat Capacity 1.21 J/g-°C
0.289 BTU/lb-°F
R&H P-37
KYDEX® 100 Acrylic/PVC Thermoplastic Sheet
High impact fire rated sheetApplications: Housings for equipment such as photocopy machines, instrument panels, computers, keyboards, telephones. Hidden parts for equipment such as vending machines..
Specific Heat Capacity 1.21 J/g-°C
0.289 BTU/lb-°F
Hippe PBT Polybutylene Terephthalate
The mechanical properties of PBT are generally inferior to the partially crystallized PET, however, PBT is more easily machined.Information provided by Hippe.
Specific Heat Capacity 1.21 J/g-°C
0.289 BTU/lb-°F
Azoty Tarnow™ TARNOFORM 300 GF4 POM
20% glass fiber reinforced injection molding grade with very high strength.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Specific Heat Capacity 1.21 J/g-°C
0.289 BTU/lb-°F
Azoty Tarnow™ TARNOFORM 300 GF6 BK POM
30% glass fiber reinforced injection molding grade, suitable for applications where increased strength and stiffness is required.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A...
Specific Heat Capacity 1.21 J/g-°C
0.289 BTU/lb-°F
Azoty Tarnow™ TARNOFORM 300 GF6 POM
30% glass fiber reinforced injection molding grade, suitable for applications where increased strength and stiffness is required.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A...
Specific Heat Capacity 1.21 J/g-°C
0.289 BTU/lb-°F
Azoty Tarnow™ TARNOFORM 300 GF7 POM
35% glass fiber reinforced injection molding grade, suitable for applications where increased strength and stiffness is required.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A...
Specific Heat Capacity 1.21 J/g-°C
0.289 BTU/lb-°F
Azoty Tarnow™ TARNOFORM 500 GF6 POM
30% glass fiber reinforced, high flow injection molding grade, suitable for applications where high strength and stiffness is required, combined with higher flowability during molding.Information pr..
Specific Heat Capacity 1.21 J/g-°C
0.289 BTU/lb-°F
3M Novec™ 7200 Engineered Fluid
3M™ Novec™ 7200 fluid's convenient boiling point and excellent environmental, health and safety profile make it useful as a heat transfer fluid, cleaning solvent, for lubricant deposition & many m..
Specific Heat Capacity 1.21 J/g-°C
0.289 BTU/lb-°F
3M Novec™ 7200DL Engineered Fluid
A high-purity version of 3M™ Novec™ 7200, 3M™ Novec™ 7200DL is tightly-controlled for ions, metals and non-volatile residue. It is used when an application calls for high-purity materials, or a ..