Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Specific Heat Capacity = 0.240 BTU/lb-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Specific Heat Capacity 1.00 J/g-°C
0.240 BTU/lb-°F
ASTM C351
Park Electrochemical Nelcote® F-554 Phenolic Prepreg, Aerospace Silica Fabric Reinforced
Nelcote® F-554 is a high purity silica filled phenolic resin coated on Commercial or Aerospace grade silica fabric. F-554 is used in the manufacture of intermediate temperature ablative rocket nozz..
Specific Heat Capacity 1.00 J/g-°C
0.240 BTU/lb-°F
ASTM C351
Park Electrochemical Nelcote® F-554 Phenolic Prepreg, Commercial Silica Fabric Reinforced
Nelcote® F-554 is a high purity silica filled phenolic resin coated on Commercial or Aerospace grade silica fabric. F-554 is used in the manufacture of intermediate temperature ablative rocket nozz..
Specific Heat Capacity 1.00 J/g-°C
0.240 BTU/lb-°F
ASTM C351
Park Electrochemical Nelcote® F-557 Phenolic Prepreg, Aerospace Silica Fabric Reinforced
Nelcote® F-557 is a high purity silica filler phonic resin coated on Commercial or Aerospace grade silica fabric. F-557 is used in the manufacture of intermediate temperature ablative rocket nozzle..
Specific Heat Capacity 1.00 J/g-°C
0.240 BTU/lb-°F
ASTM C351
Park Electrochemical Nelcote® F-557 Phenolic Prepreg, Chopped Molding Compound Reinforced
Nelcote® F-557 is a high purity silica filler phonic resin coated on Commercial or Aerospace grade silica fabric. F-557 is used in the manufacture of intermediate temperature ablative rocket nozzle..
Specific Heat Capacity 1.00 J/g-°C
0.240 BTU/lb-°F
ASTM C351
Park Electrochemical Nelcote® F-557 Phenolic Prepreg, Commercial Silica Fabric Reinforced
Nelcote® F-557 is a high purity silica filler phonic resin coated on Commercial or Aerospace grade silica fabric. F-557 is used in the manufacture of intermediate temperature ablative rocket nozzle..
Specific Heat Capacity 1.00 J/g-°C
0.240 BTU/lb-°F
DSC
Mitsui AURUM® PL450C Polyimide  (discontinued **)
AURUM PL450C is a high performance thermoplastic polyimide for precision injection molded components and extruded products. A member of the AURUM family of advanced engineering resins, unfilled AURU..
Specific Heat Capacity 1.00 J/g-°C
0.240 BTU/lb-°F
Magnesium Elektron Elektron® 21 Magnesium Casting Alloy
Fully heat treatable alloy for use up to 400°F. Excellent corrosion resistance and castability. Cast products possess a fine-grained microstructure and pressure tightness. Easily machined. Usual ..
Copyright © lookpolymers.com All Rights Reserved