Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.770 J/g-°C | 0.184 BTU/lb-°F | |
Chevron Phillips Ryton® R10 5002C PPS Polyphenylene Sulfide
(discontinued **) Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol.. |
|||
Specific Heat Capacity | 0.770 J/g-°C | 0.184 BTU/lb-°F | |
Chevron Phillips Ryton® R10 5004A PPS Polyphenylene Sulfide
(discontinued **) Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol.. |
|||
Specific Heat Capacity | 0.770 J/g-°C | 0.184 BTU/lb-°F | |
Schott K10 Glass Information Provided by SCHOTT North America, Inc. |
|||
Specific Heat Capacity | 0.770 J/g-°C | 0.184 BTU/lb-°F | |
Schott N-SF5 Glass Information Provided by SCHOTT North America, Inc. |
|||
Specific Heat Capacity | 0.770 J/g-°C | 0.184 BTU/lb-°F | |
Schott N-SF8 Glass Information Provided by SCHOTT North America, Inc. |
|||
Specific Heat Capacity | 0.770 J/g-°C | 0.184 BTU/lb-°F | |
Schott N-ZK7 Glass Information Provided by SCHOTT North America, Inc. |
|||
Specific Heat Capacity | 0.770 J/g-°C | 0.184 BTU/lb-°F | |
Schott P-PK53 Glass Suitable for precision moldingInformation Provided by SCHOTT North America, Inc. |
|||
Specific Heat Capacity | 0.768 J/g-°C | 0.184 BTU/lb-°F | |
Ceramic Process Systems AlSiC-10, 54 vol% SiC Aluminum alloy A356.2 used. Hermeticity < 1x109 atm-cc/s He.CPS fabricates AlSiC by preparing an SiC preform which is subsequently infiltrated by molten aluminum metal. After infiltration, compone.. |
|||
Specific Heat Capacity | 0.770 J/g-°C | 0.184 BTU/lb-°F | |
Chevron Phillips Ryton® R10 7006A PPS Polyphenylene Sulfide
(discontinued **) Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol.. |