Polymer Property : Specific Heat Capacity = 0.0932 BTU/lb-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Specific Heat Capacity 0.390 J/g-°C
0.0932 BTU/lb-°F
Dow Corning XIAMETER® PMCPPMX-200 5CS Silicone Fluid
Is chemically equivalent to DOW CORNING® 200 FLUID 5CS. 100% active, 5 cSt, polydimethylsiloxane polymer.Information provided by Dow Corning
Specific Heat Capacity 0.390 J/g-°C
0.0932 BTU/lb-°F
Alliance S-26B Samarium Cobalt Magnetic Material
Specific Heat Capacity 0.390 J/g-°C
0.0932 BTU/lb-°F
Alliance S-28A Samarium Cobalt Magnetic Material
Specific Heat Capacity 0.390 J/g-°C
0.0932 BTU/lb-°F
Alliance S-28B Samarium Cobalt Magnetic Material
Specific Heat Capacity 0.390 J/g-°C
0.0932 BTU/lb-°F
Alliance S-30A Samarium Cobalt Magnetic Material
Specific Heat Capacity 0.390 J/g-°C
0.0932 BTU/lb-°F
Alliance S-30B Samarium Cobalt Magnetic Material
Specific Heat Capacity 0.390 J/g-°C
0.0932 BTU/lb-°F
Alliance S-28H Samarium Cobalt Magnetic Material
Specific Heat Capacity 0.390 J/g-°C
0.0932 BTU/lb-°F
Alliance S-32 Samarium Cobalt Magnetic Material
Specific Heat Capacity 0.390 J/g-°C
0.0932 BTU/lb-°F
Alliance S-26H Samarium Cobalt Magnetic Material