Thermal Properties | Metric | English | Comments |
---|---|---|---|
Annealing Point | 70.0 - 80.0 °C | 158 - 176 °F | 3-5 hours |
LG Chemical IG840 PMMA, General Purpose Grade for Injection Molding General purpose grade with better flowability than IH 830 but slightly below in heat resistanceMechanical strength and surface hardnessFeatures: Excellent transparency and eleganceWeather resistance.. |