Polymer Property : Melting Point = 98.6 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 37.0 - 104 °C
98.6 - 219 °F
Average value: 75.4 °C Grade Count:47
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Extrusion/Coating Grade
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Extrusion/Coating Grade". Each property range of values reported..
Melting Point 37.0 °C
98.6 °F
Freezing Point via DSC/ASTM D3418
DuPont Elvax® 3185 Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion
33 wt% Vinyl Acetate.Elvax® 3185 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins..
Melting Point 37.0 °C
98.6 °F
Freezing Point; ASTM D3418, ISO 3146
DuPont™ Surlyn® 9320 Zinc Ionomer
Surlyn® 9320 is a zinc ionomer thermoplastic resin. It is available for use in conventional extrusion and injection equipment, to create various sheets or shapes. Surlyn® 9320 thermoplastic resin ..
Melting Point 37.0 °C
98.6 °F
DSC, 10°C/min (peak); DuPont Test
Dow Engage® ENX 7458.00 Ethylene-Butene Copolymer
Description: ENX 7458.00 is a unique broader molecular weight distribution ethylene-butene copolymer that offers excellent flow and impact properties and is ideally suited for plastics modification...
Melting Point 37.0 °C
98.6 °F
Freezing Point; ASTM D3418
DuPont Elvax® CM3326 Ethylene Vinyl Acetate  (discontinued **)
DuPont™ Elvax® CM3326 is an ethylene-vinyl acetate copolymer resin for use in industrial applications. Specialty grades of Elvax® have the unusual combination of high vinyl acetate levels and low..