Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melting Point = 91.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 91.0 °C
196 °F
Internal Method
Polimeri Europa Greenflex® ML 40 Ethylene Vinyl Acetate Copolymer - Injection Molding
Greenflex ML 40 is an ethylene vinyl acetate copolymer (EVA) for injection molding of flexible items. Items produced with Greenflex ML 40 show high elasticity and flexibility.Main Applications: Gr..
Melting Point 91.0 °C
196 °F
LyondellBasell Lupolen® V 3510 K Ethylene Vinyl Acetate, lnjection Molding Grade
Injection moldingsData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell.
Melting Point 91.0 °C
196 °F
LyondellBasell Lupolen® V 3520 K Ethylene Vinyl Acetate
Films, blow moldings.Data was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell.
Melting Point 91.0 °C
196 °F
By DSC; ASTM D3418 - ISO 3146
DuPont Elvaloy® 1224 AC Ethylene and 24% Methyl Acrylate Copolymer
Elvaloy® 1224 AC is intended for extrusion, coextrusion, compounding and injection molding. Elvaloy® 1224 AC has good adhesion to various substrates (OPA, OPP, paperboard, etc.), gives excellent ..
Melting Point 91.0 °C
196 °F
TRN-14
Tipco Tipcolite® TPF 1317 - Unreinforced Phenolic Resin with Minerals having 42 mm Norton Flow with 9% Hexamine
Phenolic Resin with Minerals having 42mm Norton Flow, in Powder FormApplications: Foundry & RefractoryProcessing: Castings & ShellsInformation provided by the Manufacturer, Tipco Industries Ltd., In..
Melting Point 91.0 °C
196 °F
by DSC; ASTM D3418
Westlake EBAC® SP1806 17.5%, Ethylene-Methyl Acrylate Copolymer
Description: Westlake EBAC® SP1806 is an ethylene butyl acrylate copolymer designed for extrusion coating and laminating. SP1806 can also be compounded as an impact modifier or used in highly fill..
Melting Point 91.0 °C
196 °F
ISO 11357
Total EVA 1005 VN 35 Ethylene Vinyl Acetate Copolymer - Blown Film
EVA 1005 VN 35 is made by a high pressure tubular process. Grade for flexible films, with high transparency and outstanding mechanical properties. Contains NO antioxidant.Information provided by T..
Melting Point 91.0 °C
196 °F
ISO 11357
Total EVA 1005 VN 4 Ethylene Vinyl Acetate Copolymer - Blown Film
EVA 1005 VN 4 is made by a high pressure tubular process. Grade for flexible films with high transparency and good mechanical properties. Contains an antioxidant.Application examples: High strengt..
Melting Point 91.0 °C
196 °F
Melting point via DSC/ASTM D3418
DuPont Bynel® 2002 Acid-Modified Ethylene Terpolymer Adhesive Resin
Bynel® Series 2000 resins are acid-modified ethylene terpolymers with medium to high acid comonomer contents. They contain a temperature stable ester that makes them functional in high-temperature ..
Melting Point 91.0 °C
196 °F
Freezing Point; ASTM D3418
DuPont™ Bynel® 21E781 Anhydride Modified Ethylene Acrylate
BYNEL® Series 2100 resins are anhydride modified ethylene acrylate resins. They contain a temperature stable ester which makes them functional in high temperature coextrusions. They are available i..
Melting Point 91.0 °C
196 °F
ASTM D3418, ISO 3146
DuPont™ Bynel® 22E780 Modified Ethylene Acrylate
BYNEL® Series 2200 resins are modified ethylene acrylate resins. They contain a temperature stable ester which makes them functional in high temperature coextrusions. They are available in pellet f..
Melting Point 91.0 °C
196 °F
ASTM D3418, ISO 3146
DuPont™ Entira® AS MK 400 Ionomer Resin
Entira™ AS MK400 is an extremely hygroscopic ionomer resin that is supplied as free-flowing pellets.
Melting Point 91.0 °C
196 °F
DSC
DuPont™ Surlyn® 7940 Ionomer Resin, Lithium
Surlyn® 7940 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with lithium ions. The amount of MAA and ne..