Polymer Property : Melting Point = 820 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point >= 820 °C
>= 1510 °F
Solvay Chemicals NOCOLOK® CB Flux Potassium Silicofluoride
Reactive flux for brazing of aluminumCAS-No.: 16871-90-2 Uses: Automotive Sector, Commercial & Residential Air Conditioning, Refrigeration and Household & Electrical AppliancesInformation provided ..
Melting Point 820 - 910 °C
1510 - 1670 °F
Wieland 1023 Wilaform Gold
Hard yellow gold alloy with good extensibility. Particularly suitable for by machine manufactured decoration.Applications: casting, chains, coin/shape, laminar decorationDental
Melting Point 820 - 880 °C
1510 - 1620 °F
Wieland 1101 Wilaform Gold
Hard yellow gold alloy with good extensibility. Universally applicable in decoration manufacturing.Applications: casting, chainsDental
Melting Point 820 - 890 °C
1510 - 1630 °F
Wieland 1114 Wilaform Gold
Hard yellow gold alloy with good extensibility. Universally applicable in decoration manufacturing.Applications: casting, chains, coin/shape, laminar decoration, pipes, tubingDental
Melting Point 820 - 910 °C
1510 - 1670 °F
Wieland 3013 Wilaform Silver
Universally applicable silver alloy.Applications: casting, chains, coin/shape, laminar decoration, pipes, tubingDental