Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melting Point = 592 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 311 °C
592 °F
Peak; ASTM D3418
Solvay Specialty Polymers Amodel® AT-1125 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AT-1125 HS polyphthalamide (PPA) is a toughened, heat stabilized 25% glass reinforced resin, designed as a cost effective solution for applications requiring stiffness, good dimensional stabi..
Melting Point 311 °C
592 °F
ISO 11357-3
Solvay Specialty Polymers Amodel® AT-1125 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AT-1125 HS polyphthalamide (PPA) is a toughened, heat stabilized 25% glass reinforced resin, designed as a cost effective solution for applications requiring stiffness, good dimensional stabi..
Melting Point 311 °C
592 °F
Peak; Dry; ASTM D3418
Solvay Specialty Polymers Amodel® A-1565 HS Polyphthalamide (PPA), 65% GlassMineral (Conditioned)
Amodel® A-1565 HS is a 65% glass and mineral-reinforced polyphthalamide (PPA) designed to be cost-effective in applications requiring high stiffness, good dimensional stability and good retention..
Melting Point 311 °C
592 °F
Dry; ISO 11357-3
Solvay Specialty Polymers Amodel® A-1565 HS Polyphthalamide (PPA), 65% GlassMineral (Conditioned)
Amodel® A-1565 HS is a 65% glass and mineral-reinforced polyphthalamide (PPA) designed to be cost-effective in applications requiring high stiffness, good dimensional stability and good retention..
Melting Point 311 °C
592 °F
ASTM D3418
Solvay Specialty Polymers Amodel® A-1565 HS Polyphthalamide (PPA), 65% GlassMineral (Dry)
Amodel® A-1565 HS is a 65% glass and mineral-reinforced polyphthalamide (PPA) designed to be cost-effective in applications requiring high stiffness, good dimensional stability and good retention..
Melting Point 311 °C
592 °F
ISO 11357-3
Solvay Specialty Polymers Amodel® A-1565 HS Polyphthalamide (PPA), 65% GlassMineral (Dry)
Amodel® A-1565 HS is a 65% glass and mineral-reinforced polyphthalamide (PPA) designed to be cost-effective in applications requiring high stiffness, good dimensional stability and good retention..
Melting Point 311 °C
592 °F
Peak; Dry; ASTM D3418
Solvay Specialty Polymers Amodel® AS-1566 HS Polyphthalamide (PPA), 65% GlassMineral (Conditioned)
Amodel® AS-1566 HS resin is a 65% glass and mineral reinforced polyphthalamide (PPA) resin that exhibits a high deflection temperature and high flexural modulus. This grade was designed specifica..
Melting Point 311 °C
592 °F
Dry; ISO 11357-3
Solvay Specialty Polymers Amodel® AS-1566 HS Polyphthalamide (PPA), 65% GlassMineral (Conditioned)
Amodel® AS-1566 HS resin is a 65% glass and mineral reinforced polyphthalamide (PPA) resin that exhibits a high deflection temperature and high flexural modulus. This grade was designed specifica..
Melting Point 311 °C
592 °F
ASTM D3418
Solvay Specialty Polymers Amodel® AS-1566 HS Polyphthalamide (PPA), 65% GlassMineral (Dry)
Amodel® AS-1566 HS resin is a 65% glass and mineral reinforced polyphthalamide (PPA) resin that exhibits a high deflection temperature and high flexural modulus. This grade was designed specifica..
Melting Point 311 °C
592 °F
ISO 11357-3
Solvay Specialty Polymers Amodel® AS-1566 HS Polyphthalamide (PPA), 65% GlassMineral (Dry)
Amodel® AS-1566 HS resin is a 65% glass and mineral reinforced polyphthalamide (PPA) resin that exhibits a high deflection temperature and high flexural modulus. This grade was designed specifica..
Melting Point 311 °C
592 °F
Peak; Dry; ASTM D3418
Solvay Specialty Polymers Amodel® AT-1125 HS Polyphthalamide (PPA), 25% Glass Fiber (Conditioned)
Amodel® AT-1125 HS polyphthalamide (PPA) is a toughened, heat stabilized 25% glass reinforced resin, designed as a cost effective solution for applications requiring stiffness, good dimensional s..
Melting Point 311 °C
592 °F
Dry; ISO 11357-3
Solvay Specialty Polymers Amodel® AT-1125 HS Polyphthalamide (PPA), 25% Glass Fiber (Conditioned)
Amodel® AT-1125 HS polyphthalamide (PPA) is a toughened, heat stabilized 25% glass reinforced resin, designed as a cost effective solution for applications requiring stiffness, good dimensional s..
Melting Point 311 °C
592 °F
ASTM D3418
Solvay Specialty Polymers Amodel® AT-1125 HS Polyphthalamide (PPA), 25% Glass Fiber (Dry)
Amodel® AT-1125 HS polyphthalamide (PPA) is a toughened, heat stabilized 25% glass reinforced resin, designed as a cost effective solution for applications requiring stiffness, good dimensional s..
Melting Point 311 °C
592 °F
ISO 11357-3
Solvay Specialty Polymers Amodel® AT-1125 HS Polyphthalamide (PPA), 25% Glass Fiber (Dry)
Amodel® AT-1125 HS polyphthalamide (PPA) is a toughened, heat stabilized 25% glass reinforced resin, designed as a cost effective solution for applications requiring stiffness, good dimensional s..
Melting Point 311 °C
592 °F
Peak; ASTM D3418
Solvay Specialty Polymers Amodel® A-1565 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel A-1565 HS is a 65% glass and mineral-reinforced polyphthalamide (PPA) designed to be cost-effective in applications requiring high stiffness, good dimensional stability and good retention of ..
Melting Point 311 °C
592 °F
ISO 11357-3
Solvay Specialty Polymers Amodel® A-1565 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel A-1565 HS is a 65% glass and mineral-reinforced polyphthalamide (PPA) designed to be cost-effective in applications requiring high stiffness, good dimensional stability and good retention of ..
Melting Point 311 °C
592 °F
Peak; ASTM D3418
Solvay Specialty Polymers Amodel® AS-1566 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AS-1566 HS resin is a 65% glass and mineral reinforced polyphthalamide (PPA) resin that exhibits a high deflection temperature and high flexural modulus. This grade was designed specifically ..
Melting Point 311 °C
592 °F
ISO 11357-3
Solvay Specialty Polymers Amodel® AS-1566 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AS-1566 HS resin is a 65% glass and mineral reinforced polyphthalamide (PPA) resin that exhibits a high deflection temperature and high flexural modulus. This grade was designed specifically ..
Copyright © lookpolymers.com All Rights Reserved