Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 181 - 290 °C | 358 - 554 °F | Average value: 217 °C Grade Count:3 |
Overview of materials for Polyphenylene Ether, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Molded". Each property range of values reported is minimum and maximum values of ap.. |
|||
Melting Point | 280 - 290 °C | 536 - 554 °F | Average value: 284 °C Grade Count:6 |
Overview of materials for Polyphenylene Sulfide (PPS) Alloy, Glass Reinforced, Flow Enhanced This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) Alloy, Glass Reinforced, Flow Enhanced". Each property range of values repor.. |
|||
Melting Point | 280 - 290 °C | 536 - 554 °F | Average value: 283 °C Grade Count:5 |
Overview of materials for Polyphenylene Sulfide (PPS), Conductive This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Conductive". Each property range of values reported is minimum and maximum .. |
|||
Melting Point | 260 - 290 °C | 500 - 554 °F | |
Guarniflon MFA Fluoropolymer It’s a semi-crystalline fully-fluorinated melt processable fluoropolymer which offer the highest temperature rating and broadest chemical resistance of all melt processable fluoropolymers. It .. |
|||
Melting Point | 280 - 290 °C | 536 - 554 °F | DSC |
Solvay Specialty Polymers Hyflon® MFA® P6010 Perfluoropolymer Hyflon® MFA P6010 is a clear, semi-crystalline melt processable perfluorinated resin. It is designed for electrostatic powder coatings and is particularly recommended for use as a topcoat in anti.. |
|||
Melting Point | 280 - 290 °C | 536 - 554 °F | DSC |
Solvay Specialty Polymers Hyflon® MFA® P6310 Perfluoropolymer Hyflon® MFA P6310 is a clear, semi-crystalline melt processable perfluorinated resin. It is designed for electrostatic powder coatings and is particularly recommended for use as a topcoat in anti.. |
|||
Melting Point | 280 - 290 °C | 536 - 554 °F | DSC |
Solvay Specialty Polymers Hyflon® PFA M620 Perfluoroalkoxy (PFA) Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat res.. |
|||
Melting Point | 280 - 290 °C | 536 - 554 °F | DSC |
Solvay Specialty Polymers Hyflon® PFA M640 Perfluoroalkoxy (PFA) Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat res.. |
|||
Melting Point | 280 - 290 °C | 536 - 554 °F | DSC |
Solvay Specialty Polymers Hyflon® MFA® 1041 Perfluoropolymer Hyflon® MFA 1041 is a high extrusion speed resin specifically designed for insulation for plenum-rated LAN cables. MFA 1041 delivers superior electrical performance in addition to its excellent f.. |
|||
Melting Point | 268 - 290 °C | 514 - 554 °F | |
Williams Advanced Alloys WS290 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Melting Point | 280 - 290 °C | 536 - 554 °F | |
A. Schulman ComAlloy E-16674B PPS, Electrically Conductive - Carbon Fiber Filled Data provided by the manufacturer, ComAlloy International Company.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Melting Point | 280 - 290 °C | 536 - 554 °F | |
A. Schulman ComAlloy E-16769N Internally Lubricated, Glass Fiber Reinforced PPS Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma.. |
|||
Melting Point | 280 - 290 °C | 536 - 554 °F | |
A. Schulman ComAlloy Hiloy® 714 PPS, Glass Reinforced, UL Data provided by the manufacturer, ComAlloy International Company.40% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Melting Point | 280 - 290 °C | 536 - 554 °F | |
A. Schulman ComAlloy Hiloy® 754 Glass Reinforced, Flow Enhanced, PPS Alloy, UL Data provided by the manufacturer, ComAlloy International Company.40% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Melting Point | 280 - 290 °C | 536 - 554 °F | |
A. Schulman ComAlloy Hiloy® 758 Carbon Fiber Reinforced, Flow Enhanced, PPS Alloy Data provided by the manufacturer, ComAlloy International Company.40% Carbon Fiber Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has b.. |
|||
Melting Point | 280 - 290 °C | 536 - 554 °F | |
A. Schulman ComAlloy E-16901B PPS Alloy, Electrically Conductive - Carbon Fiber Filled Data provided by the manufacturer, ComAlloy International Company.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Melting Point | 280 - 290 °C | 536 - 554 °F | |
A. Schulman ComAlloy E-16902N PPS Alloy, Electrically Conductive - Stainless Steel Fiber Filled Data provided by the manufacturer, ComAlloy International Company.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Melting Point | 280 - 290 °C | 536 - 554 °F | |
A. Schulman ComAlloy Hiloy® 753 Glass Reinforced, Flow Enhanced, PPS Alloy, UL Data provided by the manufacturer, ComAlloy International Company.30% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Melting Point | 280 - 290 °C | 536 - 554 °F | |
A. Schulman ComAlloy Hiloy® 757 Carbon Fiber Reinforced, Flow Enhanced, PPS Alloy Data provided by the manufacturer, ComAlloy International Company.30% Carbon Fiber Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Melting Point | 280 - 290 °C | 536 - 554 °F | ASTM D3307 |
Solvay Specialty Polymers Hyflon® PFA M620 Perfluoroalkoxy (PFA)
(Unverified Data**) Hyflon PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resista.. |
|||
Melting Point | 280 - 290 °C | 536 - 554 °F | ASTM D3307 |
Solvay Specialty Polymers Hyflon® PFA M640 Perfluoroalkoxy (PFA)
(Unverified Data**) Hyflon PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resista.. |
|||
Melting Point | 280 - 290 °C | 536 - 554 °F | |
A. Schulman ComAlloy Hiloy® 716 PPS, Carbon Fiber Reinforced Data provided by the manufacturer, ComAlloy International Company.20% Carbon Fiber Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Melting Point | 280 - 290 °C | 536 - 554 °F | |
A. Schulman ComAlloy Hiloy® 756 Carbon Fiber Reinforced, Flow Enhanced, PPS Alloy Data provided by the manufacturer, ComAlloy International Company.20% Carbon Fiber Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Melting Point | 280 - 290 °C | 536 - 554 °F | ASTM D-3418 |
Saint-Gobain Norton® MFA Fluoropolymer Film Features/Benefits:Outstanding clarityPerformance from -254°C (-425°F) to 230°C (446°F)Outstanding flex life and stress-crack resistanceOutstanding anti-stick release propertiesExcellent electric.. |