Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 235 - 263 °C | 455 - 505 °F | Average value: 254 °C Grade Count:9 |
Overview of materials for Nylon 66/Nylon 6 Blend, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/Nylon 6 Blend, Glass Fiber Filled". Each property range of values reported is minimum and maxim.. |
|||
Melting Point | 255 - 263 °C | 491 - 505 °F | Average value: 259 °C Grade Count:65 |
Overview of materials for Nylon 66, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and ma.. |
|||
Melting Point | 221 - 263 °C | 430 - 505 °F | Average value: 256 °C Grade Count:11 |
Overview of materials for Nylon 66, 30% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Carbon Fiber Filled". Specific grades with carbon fiber content between 25% and 34% are in.. |
|||
Melting Point | 184 - 263 °C | 363 - 505 °F | |
Indium Corp. Indalloy 144 Tin-Lead Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 255 - 263 °C | 491 - 505 °F | Average value: 259 °C Grade Count:11 |
Overview of materials for Nylon 66, 20% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are inclu.. |