Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 182 - 187 °C | 360 - 369 °F | Average value: 184 °C Grade Count:8 |
Overview of materials for Nylon 11, Cable Sheathing Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11, Cable Sheathing Grade". Each property range of values reported is minimum and maximum values o.. |
|||
Melting Point | 183 - 187 °C | 361 - 369 °F | |
Hong Kun Group AO 168 Antioxidant CAS No. 31570-04-4All information provided by Hongkun Group |
|||
Melting Point | 175 - 187 °C | 347 - 369 °F | Huntsman/TMA |
Huntsman IROGRAN® A 92 E 4738 Polyester-Based TPU-Injection Extrusion Grade Introduction: IROGRAN A 92 E 4738 is a white-colored, thermoplastic special-polyester-polyurethane for injection molding applications. Additional characteristics of the product are flexibility and h.. |
|||
Melting Point | 181 - 187 °C | 358 - 369 °F | |
Indium Corp. Indalloy 226 Tin Solder Alloy Zinc causes high dross U.S. Patent #5,242,658; covers 72.8-89.4Sn 6.7-19.2Zn 2.7-16.4In; temp. range Liq.. 176-193, Sol. 166-191.4Information Provided by Indium Corporation |
|||
Melting Point | 175 - 187 °C | 347 - 369 °F | |
Indium Corp. Indalloy® 227 Sn-In-Ag Solder Alloy Pb free solder can be used as a replacement for 63Sn 37Pb, 62Sn 36Pb 2Ag and 60Sn 40Pb in that it has similar physical and mechanical properties. Not for use over 100°C due to 118°C Sn/In eut.. |
|||
Melting Point | 183 - 187 °C | 361 - 369 °F | |
Suqian Unitechem Antioxidant 168 Chemical Name: Tris-(2,4-di-tert-butyl-phenyl)-phosphiteCAS NO.: 31570-04-4Molecular Formula: C42H63O3PProperties: The product takes on an appearance of white powder, without odor and smell. Solubl.. |
|||
Melting Point | 175 - 187 °C | 347 - 369 °F | |
Williams Advanced Alloys WS187 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |