Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 165 - 173 °C | 329 - 344 °F | Average value: 166 °C Grade Count:15 |
Overview of materials for Acetal Copolymer, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% ar.. |