Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 170 °C | 338 °F | ISO 11357-1 |
Murtfeldt Murytal® C Blue [FS] Acetal Copolymer Thanks to their extremely low absorption of moisture, Murytal® materials are ideally suited for use as electronic isolation components. A fine crystalline structure and high yield strength mean th.. |
|||
Melting Point | 170 °C | 338 °F | |
Nylacast POM C Acetal Copolymer The copolymer grade is the ideal combination of strength, stiffness and wears resistance. It absorbs very little moisture, is easily machinable and is genuinely porosity-free making it the preferred.. |
|||
Melting Point | 170 °C | 338 °F | |
Hybrid Plastics Polyamide POSS® Flow Masterbatch POSS® Flow masterbatches show success in reducing the melt viscosity of a variety of injection molded and extruded resins. Hybrid Plastics now introduces such a solution for polyamide polymers. P.. |
|||
Melting Point | 170 °C | 338 °F | DIN 53736; ASTM D789 |
Kolon KOLEFIN® KO133MT40 M/F Reinforced Polypropylene KOLEFIN® has excellent mechanical properties and its cost is lower than other engineering plastics. KOLEFIN® is widely used in the automotive industry and business applications.Good mechanica.. |
|||
Melting Point | 170 - 185 °C | 338 - 365 °F | Huntsman/TMA |
Huntsman IROGRAN® A 92 H 4656 Polyester-Based TPU-Injection Molding Grade Introduction: IROGRAN A 92 H 4656 is a thermoplastic polyester- polyurethane for injection molding applications. Additional characteristics of the product are short cycle times, good melt flow and e.. |
|||
Melting Point | 170 - 175 °C | 338 - 347 °F | ASTM D789 |
Lucent Polymers POM-900P Acetal Homopolymer, Easy Flow, Injection Grade Add "U" for UV StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Melting Point | 170 - 174 °C | 338 - 345 °F | DSC |
Solvay Specialty Polymers Solef® 6012 Polyvinylidene Fluoride (PVDF) Solef® 6012 PVDF homopolymer is a high-viscosity PVDF resin and is typically processed by extrusion or compression molding.Features: High Viscosity; HomopolymerAdditional Properties: Crystallizat.. |
|||
Melting Point | 170 °C | 338 °F | |
Techmer ES HiFill® PP GB10 10% Glass Beads Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 10% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Melting Point | 170 °C | 338 °F | |
Techmer ES HiFill® PP GB20 20% Glass Beads Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 20% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Melting Point | 170 °C | 338 °F | |
Techmer ES HiFill® PP GB30 30% Glass Beads Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 30% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Melting Point | 170 °C | 338 °F | |
Techmer ES HiFill® PP GB60 60% Glass Beads Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 60% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Melting Point | 170 °C | 338 °F | |
Unitika TERRAMAC TE-8210 Polylactic Acid (PLA) High-durability, Injection grade. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd. |
|||
Melting Point | 170 °C | 338 °F | DSC |
Toyobo Pelprene™ P-150M Polyester TPE Key Feature: Pelprene P typePelprene™ can be processed into a wide variety of articles from ultra-small precision parts to sheets by injection, extrusion, and blow molding. The 'P' type is a block.. |
|||
Melting Point | 170 °C | 338 °F | DSC |
Lubrizol Estane® 58246 Thermoplastic Polyurethane Features: High stiffness grade with excellent chemical and oil resistance.Uses: Flat Die/Cast Film Extrusion and Injection Molding.Available in Americas, Europe, Middle East, Africa, India and AsiaI.. |
|||
Melting Point | 170 °C | 338 °F | |
Unitika TERRAMAC HV-6250H Polylactic Acid (PLA) Foam, Extrusion, blow, and foam sheet grades. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd. |
|||
Melting Point | 170 °C | 338 °F | |
Unitika TERRAMAC TE-1030 Polylactic Acid (PLA) High-Impact grade, Injection grade. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd. |
|||
Melting Point | 170 °C | 338 °F | |
Unitika TERRAMAC TE-7000 Polylactic Acid (PLA) Heat-resisting grade, Injection grade. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd. |
|||
Melting Point | 170 °C | 338 °F | |
Unitika TERRAMAC TE-7300 Polylactic Acid (PLA) Heat-resisting grade, Injection grade. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd. |
|||
Melting Point | 170 °C | 338 °F | |
Unitika TERRAMAC TE-8300 Polylactic Acid (PLA) High-durability, Injection grade. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd. |
|||
Melting Point | 170 °C | 338 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® XE 3982 PA12 Product description: Grilamid XE 3982 is a highly flexible extrusion grade, based on Polyamide 12 with following main attributes: High flexibilityLow plasticizer migration (low blooming)Very good ch.. |
|||
Melting Point | 170 °C | 338 °F | (Dry) |
Arkema Group Pebax® MV 1041 SN 01 Polyether Block Amide (PEBA) (Conditioned) POLYETHER BLOCK AMIDE (PEBA) hardness 60 shore D breathable (high permeability to H2O vapor,CO2,O2) permanent antistatic grade Applications: breathable films (medical, textile....)ISO data provided .. |
|||
Melting Point | 170 °C | 338 °F | (Dry) |
Arkema Group Rilsan® BESN F15 TL Nylon 11, Flexible Tubing Grade (Conditioned) Designation ISO 1874-PA11-P,EHL,16-001High flexible grade for tubes extrusion. Available color: black and natural. Light and heat stabilized.High flexibility. High burst pressure and impact strength.. |
|||
Melting Point | 170 °C | 338 °F | 10°C/min.; ISO 3146 |
Azoty Tarnow™ TARNOFORM 411 POM Easy flowing, internally strengthened grade for injection molding of thin walled parts of very high mechanical requirements.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Melting Point | 170 °C | 338 °F | 10°C/min; ISO 11357-1/-3 |
Barlog Plastics KEBAFLEX P D40.3 Polyester-Elastomer, Shore D40 TPC-ETInformation provided by BARLOG plastics GmbH. |
|||
Melting Point | 170 - 174 °C | 338 - 345 °F | ASTM D3418 |
Solvay Specialty Polymers Solef® 60512 Polyvinylidene Fluoride (PVDF)