Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 324 °C | 615 °F | Peak; ASTM D3418 |
Solvay Specialty Polymers Amodel® A-4122 NL WH 905 Polyphthalamide (PPA)
(Unverified Data**) Amodel A-4122 NL resin is a 22% glass reinforced, high-reflectivity white grade of polyphthalamide (PPA), designed to provide high crystallinity when molded in water-cooled molds. This material exhi.. |
|||
Melting Point | 324 °C | 615 °F | ISO 11357-3 |
Solvay Specialty Polymers Amodel® A-4422 LS WH118 Polyphthalamide (PPA)
(Unverified Data**) Amodel A-4422 LS resin is a 22% reinforced, light-stabilized, high-reflectivity white grade of polyphthalamide (PPA). The material exhibits high heat resistance, high strength and stiffness over a b.. |
|||
Melting Point | 324 °C | 615 °F | ASTM D3418 |
Solvay Specialty Polymers Amodel® A-4122 NL WH 905 Polyphthalamide (PPA), 22% Glass Fiber Amodel® A-4122 NL resin is a 22% glass reinforced, high-reflectivity white grade of polyphthalamide (PPA), designed to provide high crystallinity when molded in water-cooled molds. This material .. |
|||
Melting Point | 324 °C | 615 °F | ISO 11357-3 |
Solvay Specialty Polymers Amodel® A-4422 LS WH118 Polyphthalamide (PPA), 22% Mineral Amodel® A-4422 LS resin is a 22% reinforced, light-stabilized, high-reflectivity white grade of polyphthalamide (PPA). The material exhibits high heat resistance, high strength and stiffness over.. |
|||
Melting Point | 324 °C | 615 °F | ISO 3146 |
ExxonMobil PP1055E2 Polypropylene Homopolymer Product Description: A nucleated homopolymer resin with good flowability and antistatic properties. It is designed for molding of media packaging, containers and other articles requiring fast moldi.. |
|||
Melting Point | 324 °C | 615 °F | ISO 3146 |
ExxonMobil PP7054L1 Polypropylene Impact Copolymer Product Description: A nucleated impact copolymer resin with medium flow. It is suitable for molding applications like consumer products, closures, containers, toys and rigid packaging applications.. |
|||
Melting Point | 324 °C | 615 °F | ISO 3146 |
ExxonMobil PP7075L1 Polypropylene Impact Copolymer Product Description: A nucleated impact copolymer resin with high flow and antistatic properties. It is suitable for molding applications like disposable houseware, consumer products, toys and rigi.. |
|||
Melting Point | 324 °C | 615 °F | ISO 3146 |
ExxonMobil PP7064L1 Polypropylene Impact Copolymer Product Description: A nucleated impact copolymer resin with medium flow, high stiffness and antistatic properties. It is suitable for molding applications like consumer products, closures, contain.. |