Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 320 - 330 °C | 608 - 626 °F | ISO 11357-3 |
PolyOne Edgetek® AM-35GF/000 FR NH Polyphthalamide (PPA) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Melting Point | 320 - 325 °C | 608 - 617 °F | |
Solvay Specialty Polymers Polymist® F-5 PTFE Powder Lubricant
(discontinued **) Polymist® powders are a family of white free-flowing polytetrafluoroethylene powders for use as additives in other materials to enhance processing or end-use performance characteristics. Polymist .. |
|||
Melting Point | 320 - 340 °C | 608 - 644 °F | Average value: 328 °C Grade Count:22 |
Overview of materials for Polytetrafluoroethylene (PTFE) Powder This property data is a summary of similar materials in the MatWeb database for the category "PTFE Powder". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |
|||
Melting Point | 320 - 340 °C | 608 - 644 °F | Melting Range; DTA |
Fluorseals PTFE Unfilled Information provided by TEKU GmbH Fluorkunststoffe, a distributor of Fluorseals materials. |
|||
Melting Point | 320 °C | 608 °F | |
Mitsui Arlen™ A315 15% Glass Fiber-Reinforced Modified Nylon 6T (DAM) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss.. |
|||
Melting Point | 320 °C | 608 °F | |
Mitsui Arlen™ A335 35% Glass Fiber-Reinforced Modified Nylon 6T (COND) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss.. |
|||
Melting Point | 320 °C | 608 °F | |
Mitsui Arlen™ A335 35% Glass Fiber-Reinforced Modified Nylon 6T (DAM) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss.. |
|||
Melting Point | 320 °C | 608 °F | |
Mitsui Arlen™ A350 50% Glass Fiber-Reinforced Modified Nylon 6T (COND) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss.. |
|||
Melting Point | 320 °C | 608 °F | |
Mitsui Arlen™ AE4200 Modified Nylon 6T, for Tribolic Applications (COND) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss.. |
|||
Melting Point | 320 °C | 608 °F | |
Mitsui Arlen™ AE4200N Modified Nylon 6T, for Tribolic Applications, Flame Retardant (DAM) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss.. |
|||
Melting Point | 320 - 330 °C | 608 - 626 °F | DSC |
Solvay Specialty Polymers Algoflon® L100 Polytetrafluoroethylene (PTFE) Algoflon® L100 a white PTFE micronized powder produced from dispersion polymerization comprising loose agglomerates of sub-micron sized primary particles. Algoflon® L100 can be de-agglomerated.. |
|||
Melting Point | 320 - 330 °C | 608 - 626 °F | ASTM D3418 |
Solvay Specialty Polymers Algoflon® L600 Polytetrafluoroethylene (PTFE) Algoflon® L600 a white PTFE micronized powder produced from dispersion polymerization comprising loose agglomerates of sub-micron sized primary particles. Algoflon® L600 can be de-agglomerated.. |
|||
Melting Point | 320 °C | 608 °F | Dry; ISO 11357-3 |
Solvay Specialty Polymers Amodel® AS-4145 HS Polyphthalamide (PPA), 45% Glass Fiber (Conditioned) Amodel® AS-4145 HS polyphthalamide (PPA) is a 45% glass reinforced resin that is hot-water moldable. Key properties include high heat resistance, high strength and stiffness over a broad tempera.. |
|||
Melting Point | 320 °C | 608 °F | ISO 11357-3 |
Solvay Specialty Polymers Amodel® AS-4145 HS Polyphthalamide (PPA), 45% Glass Fiber (Dry) Amodel® AS-4145 HS polyphthalamide (PPA) is a 45% glass reinforced resin that is hot-water moldable. Key properties include high heat resistance, high strength and stiffness over a broad tempera.. |
|||
Melting Point | 320 - 330 °C | 608 - 626 °F | ASTM-D-4591 |
Shamrock Technologies Fluoro FR-150 Anti-dripping Thermoplastic Grade PTFE Additive The addition of micronized polytetrafluoroethylene (PTFE) powder to polymeric resins (and to polymeric resins containing glass fiber) provides greatly increased resistance to surface wear and abrasi.. |
|||
Melting Point | 320 - 330 °C | 608 - 626 °F | ASTM-D-4591 |
Shamrock Technologies Fluoro T® 615 Thermoplastic Grade PTFE Additive The addition of micronized polytetrafluoroethylene (PTFE) powder to polymeric resins provides greatly increased resistance to surface wear and abrasion. PTFE has a very low coefficient of friction .. |
|||
Melting Point | 320 - 330 °C | 608 - 626 °F | ASTM-D-4591 |
Shamrock Technologies Fluoro T® 715 Thermoplastic Grade PTFE Additive The addition of micronized polytetrafluoroethylene (PTFE) powder to polymeric resins provides greatly increased resistance to surface wear and abrasion. PTFE has a very low coefficient of friction .. |
|||
Melting Point | 320 - 330 °C | 608 - 626 °F | ASTM-D-4591 |
Shamrock Technologies Fluoro T® 807 Thermoplastic Grade PTFE Additive The addition of micronized polytetrafluoroethylene (PTFE) powder to polymeric resins provides greatly increased resistance to surface wear and abrasion. PTFE has a very low coefficient of friction .. |
|||
Melting Point | 320 - 330 °C | 608 - 626 °F | ASTM-D-4591 |
Shamrock Technologies Fluoro T® 811 Thermoplastic Grade PTFE Additive The addition of micronized polytetrafluoroethylene (PTFE) powder to polymeric resins provides greatly increased resistance to surface wear and abrasion. PTFE has a very low coefficient of friction .. |
|||
Melting Point | 320 - 330 °C | 608 - 626 °F | ASTM-D-4591 |
Shamrock Technologies Fluoro T® 815 Thermoplastic Grade PTFE Additive The addition of micronized polytetrafluoroethylene (PTFE) powder to polymeric resins provides greatly increased resistance to surface wear and abrasion. PTFE has a very low coefficient of friction .. |
|||
Melting Point | 320 - 330 °C | 608 - 626 °F | ASTM-D-4591 |
Shamrock Technologies MicroFLON® 1253 Thermoplastic Grade PTFE Additive Special grade for fine dispersion.The addition of micronized polytetrafluoroethylene (PTFE) powder to polymeric resins provides greatly increased resistance to surface wear and abrasion. PTFE has a.. |
|||
Melting Point | 320 - 330 °C | 608 - 626 °F | ASTM-D-4591 |
Shamrock Technologies Fluoro T® 602 Thermoplastic Grade PTFE Additive The addition of micronized polytetrafluoroethylene (PTFE) powder to polymeric resins provides greatly increased resistance to surface wear and abrasion. PTFE has a very low coefficient of friction .. |
|||
Melting Point | 320 - 330 °C | 608 - 626 °F | ASTM-D-4591 |
Shamrock Technologies Fluoro T® 603 Thermoplastic Grade PTFE Additive The addition of micronized polytetrafluoroethylene (PTFE) powder to polymeric resins provides greatly increased resistance to surface wear and abrasion. PTFE has a very low coefficient of friction .. |
|||
Melting Point | 320 °C | 608 °F | DSC |
Wolf Kunststoff ZEDEX® ZX-530CD3 031 Polymer Alloy, Fiber Reinforced and PTFE Modified Main Characteristics: Dimensionally stable and rigid; Stress resistant; Extremely low wear to 100 ° CApplications: Chemical Engineering; Laboratory Technology; Automitve Technology; Machine ToolsIn.. |
|||
Melting Point | 320 °C | 608 °F | ISO 3146 |
ExxonMobil PP1064L1 Polypropylene Homopolymer Product Description: A homopolymer resin designed for general use. It is suitable for masterbatch carrier and other compounding applications and for the molding of caps, cups, containers and other .. |
|||
Melting Point | 320 °C | 608 °F | ISO 11357-3 |
Solvay Specialty Polymers Amodel® AS-4145 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-4145 HS polyphthalamide (PPA) is a 45% glass reinforced resin that is hot-water moldable. Key properties include high heat resistance, high strength and stiffness over a broad temperature.. |
|||
Melting Point | 320 °C | 608 °F | ASTM D570 |
Solvay Specialty Polymers Amodel® AS-4145 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-4145 HS polyphthalamide (PPA) is a 45% glass reinforced resin that is hot-water moldable. Key properties include high heat resistance, high strength and stiffness over a broad temperature.. |