Polymer Property : Melting Point = 270 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 184 - 270 °C
363 - 518 °F
Indium Corp. Indalloy 146 Lead Solder Alloy
Information Provided by Indium Corporation
Melting Point 260 - 270 °C
500 - 518 °F
Guarniflon FEP Fluorinated Ethylene Propylene
Fluorinated thermoplastic material with excellent thermal, electrical and chemical inertness properties. Widely used for different industrial applications for its excellent chemical resistance up t..
Melting Point 255 - 270 °C
491 - 518 °F
DSC
Solvay Specialty Polymers Hyflon® PFA C920-0020X Perfluoroalkoxy (PFA)
Hyflon® PFA C920-0020X is a semi crystalline, melt processable perfluoroalkoxy fluorocarbon resin specifically designed for applications where the unique properties of PFAs must be combined with ..
Melting Point 250 - 270 °C
482 - 518 °F
ASTM D-3418
Saint-Gobain Norton® ETFE Fluoropolymer Film
Features/Benefits:Superior release propertiesExcellent weatherabilityPerformance from -200°C (-328°F) to 165°C (330°F)Excellent chemical and mechanical propertiesThermoformableProduct th..
Melting Point 220 - 270 °C
428 - 518 °F
Tisan TISBLEND® PC/ABS
TISBLEND has a wide area of application in electric/electronic, food packaging, information technology, information technology, medical and automotive industries. General Specification include: High..
Melting Point 260 - 270 °C
500 - 518 °F
Daikin NEOFLON NP-120 FEP Pellets
NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding.Applications: Heavy wall wire insulation, cable jacketing, tubes..
Melting Point 260 - 270 °C
500 - 518 °F
Daikin NEOFLON NP-21 FEP Pellets
NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding, injection molding.Applications: Suited to high speed extrusion ..