Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 1265 - 1354 °C | 2309 - 2469 °F | |
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, 15.9 mm thick bar Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and.. |
|||
Melting Point | 1265 - 1354 °C | 2309 - 2469 °F | |
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, air cooled, 1.0 mm thick sheet Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and.. |
|||
Melting Point | 1265 - 1354 °C | 2309 - 2469 °F | |
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, air cooled, 11.1 mm thick plate Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and.. |
|||
Melting Point | 1265 - 1354 °C | 2309 - 2469 °F | |
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, air cooled, 15.9 mm thick plate Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and.. |
|||
Melting Point | 1265 - 1354 °C | 2309 - 2469 °F | |
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, air cooled, 15.9 mm thick plate, aged 3 hours at 816°C Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and.. |
|||
Melting Point | 1265 - 1354 °C | 2309 - 2469 °F | |
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, air cooled, 4.8 mm thick sheet Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and.. |
|||
Melting Point | 1288 - 1354 °C | 2350 - 2469 °F | |
Haynes Multimet® alloy, 1.32 mm thick sheet, 1177°C heat treatment, rapid air cooled Recommended for use in applications involving high stress at temperatures up to 816°C (1500°F), and moderate stresses up to 1093°C (2000°F). Excellent oxidation resistance, good ductilit.. |
|||
Melting Point | 1288 - 1354 °C | 2350 - 2469 °F | |
Haynes Multimet® alloy, 6.15 mm hot-rolled bar, 1185°C heat treatment, rapid air cooled Recommended for use in applications involving high stress at temperatures up to 816°C (1500°F), and moderate stresses up to 1093°C (2000°F). Excellent oxidation resistance, good ductilit.. |
|||
Melting Point | 1288 - 1354 °C | 2350 - 2469 °F | |
Haynes Multimet® alloy, 6.15 mm hot-rolled bar, 15% cold reduction Recommended for use in applications involving high stress at temperatures up to 816°C (1500°F), and moderate stresses up to 1093°C (2000°F). Excellent oxidation resistance, good ductilit.. |
|||
Melting Point | 1288 - 1354 °C | 2350 - 2469 °F | |
Haynes Multimet® alloy, 6.15 mm hot-rolled bar, 30% cold reduction Recommended for use in applications involving high stress at temperatures up to 816°C (1500°F), and moderate stresses up to 1093°C (2000°F). Excellent oxidation resistance, good ductilit.. |
|||
Melting Point | 1288 - 1354 °C | 2350 - 2469 °F | |
Haynes Multimet® alloy, 6.15 mm hot-rolled bar, 40% cold reduction Recommended for use in applications involving high stress at temperatures up to 816°C (1500°F), and moderate stresses up to 1093°C (2000°F). Excellent oxidation resistance, good ductilit.. |
|||
Melting Point | 1288 - 1354 °C | 2350 - 2469 °F | |
Haynes Multimet® alloy, 6.15 mm hot-rolled bar, 5% cold reduction Recommended for use in applications involving high stress at temperatures up to 816°C (1500°F), and moderate stresses up to 1093°C (2000°F). Excellent oxidation resistance, good ductilit.. |
|||
Melting Point | 1288 - 1354 °C | 2350 - 2469 °F | |
Haynes Multimet® alloy, GTAW, 9.5 mm plate Recommended for use in applications involving high stress at temperatures up to 816°C (1500°F), and moderate stresses up to 1093°C (2000°F). Excellent oxidation resistance, good ductilit.. |
|||
Melting Point | 1288 - 1354 °C | 2350 - 2469 °F | |
Haynes Multimet® alloy, SMAW, 12.7 mm plate Recommended for use in applications involving high stress at temperatures up to 816°C (1500°F), and moderate stresses up to 1093°C (2000°F). Excellent oxidation resistance, good ductilit.. |
|||
Melting Point | 1332 - 1354 °C | 2430 - 2469 °F | |
Haynes Ultimet® alloy, 12.7 mm (1/2 in.) thick plate, SMAW weld Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Melting Point | 1332 - 1354 °C | 2430 - 2469 °F | |
Haynes Ultimet® alloy, 12.7-50.8 mm bar Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Melting Point | 1332 - 1354 °C | 2430 - 2469 °F | |
Haynes Ultimet® alloy, 6.3-38.1 mm plate Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Melting Point | 1332 - 1354 °C | 2430 - 2469 °F | |
Haynes Ultimet® alloy, aged 1000 hours at 204°C (400°F) Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Melting Point | 1332 - 1354 °C | 2430 - 2469 °F | |
Haynes Ultimet® alloy, aged 1000 hours at 316°C Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Melting Point | 1332 - 1354 °C | 2430 - 2469 °F | |
Haynes Ultimet® alloy, aged 1000 hours at 538°C (1000°F) Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Melting Point | 1332 - 1354 °C | 2430 - 2469 °F | |
Haynes Ultimet® alloy, aged 1000 hours at 760°C (1400°F) Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Melting Point | 1332 - 1354 °C | 2430 - 2469 °F | |
Haynes Ultimet® alloy, aged 1000 hours at 982°C Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Melting Point | 1332 - 1354 °C | 2430 - 2469 °F | |
Haynes Ultimet® alloy, all-weld metal, SMAW weld Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Melting Point | 1332 - 1354 °C | 2430 - 2469 °F | |
Haynes Ultimet® alloy, mill annealed Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Melting Point | 1332 - 1354 °C | 2430 - 2469 °F | |
Haynes Ultimet® alloy, plate, GMAW weld (short) Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Melting Point | 1332 - 1354 °C | 2430 - 2469 °F | |
Haynes Ultimet® alloy, plate, GMAW weld (spray) Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Melting Point | 1288 - 1354 °C | 2350 - 2469 °F | |
Haynes Multimet® alloy, 6.15 mm hot-rolled bar, 35% cold reduction Recommended for use in applications involving high stress at temperatures up to 816°C (1500°F), and moderate stresses up to 1093°C (2000°F). Excellent oxidation resistance, good ductilit.. |
|||
Melting Point | 1288 - 1354 °C | 2350 - 2469 °F | |
Haynes Multimet® alloy, SMAW, 9.5 mm plate Recommended for use in applications involving high stress at temperatures up to 816°C (1500°F), and moderate stresses up to 1093°C (2000°F). Excellent oxidation resistance, good ductilit.. |
|||
Melting Point | 1288 - 1354 °C | 2350 - 2469 °F | |
Haynes Multimet® alloy, 533.4 by 82.55 mm forging, stress relieved at 649°C (1200°F), air cooled Recommended for use in applications involving high stress at temperatures up to 816°C (1500°F), and moderate stresses up to 1093°C (2000°F). Excellent oxidation resistance, good ductility, and i.. |
|||
Melting Point | 1265 - 1354 °C | 2309 - 2469 °F | |
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, air cooled, 11.1 mm thick plate, aged 3 hours at 816°C Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and.. |