Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 114 °C | 238 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil LD 117.03 Blown Overwrap Film Resin
(discontinued **) LD 117 resins are homopolymer film resins with good clarity and excellent stiffness. Film from LD 117 resins can be used in overwrap applications and push-through type packaging equipment. Film ma.. |
|||
Melting Point | 114 °C | 238 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil LD 117.08 Blown Overwrap Film Resin
(discontinued **) LD 117 resins are homopolymer film resins with good clarity and excellent stiffness. Film from LD 117 resins can be used in overwrap applications and push-through type packaging equipment. Film ma.. |