Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 101 °C | 214 °F | Internal Method |
Polimeri Europa Greenflex® ML 20 Ethylene Vinyl Acetate Copolymer - Injection Molding Greenflex ML 20 is an ethylene vinyl acetate copolymer (EVA) for injection molding, when a good ESCR is required.Main Applications: Greenflex ML 20 is recommended for the production of flexible ite.. |
|||
Melting Point | 101 °C | 214 °F | Internal Method |
Polimeri Europa Greenflex® ML 21 Ethylene Vinyl Acetate Copolymer - Injection Molding Greenflex ML 21 is an ethylene vinyl acetate copolymer (EVA) for injection molding, when a good ESCR is required. Greenflex ML 21 contains additive waxes to obtain high production speed.Main Applic.. |
|||
Melting Point | 101 °C | 214 °F | 10°C/min; ASTM D3418 |
LG Chemical SEETEC EF320 Ethylene Vinyl Acetate Characteristics: Good Mechanical Properties and Good Optical PropertiesApplications: Agricultural FilmCAS No. 24937-78-8Information provided by LG Chemical |
|||
Melting Point | 101 - 105 °C | 214 - 221 °F | |
Suqian Unitechem UV320 (UV5411) Chemical Name: 2-(2'-Hydroxy-5'-tert-octylphenyl) benzotriazoleCAS NO.: 3147-75-9Molecular Formula: C20H25N3OInformation Provided by Suqian Unitechem Co., Ltd. |
|||
Melting Point | 101 °C | 214 °F | Freezing point via DSC/ASTM D3418 |
DuPont Bynel® 50E571 Anhydride-Modified Polypropylene Adhesive Resin Bynel® Series 5000 resins are anhydride-modified polypropylene. Bynel® 50E561 and 50E571 are based on polypropylene random copolymers. They are available in pellet form for use in conventional ext.. |
|||
Melting Point | 101 °C | 214 °F | By DSC; ASTM D3418 - ISO 3146 |
DuPont Elvaloy® 1209 AC Ethylene and 9% Methyl Acrylate Copolymer Elvaloy® 1209 AC is intended for film coextrusion and injection molding. It can be recommended in film applications where softness, flexibility and excellent sealing properties are needed.Elvaloy®.. |
|||
Melting Point | 101 °C | 214 °F | By DSC; ASTM D3418 - ISO 3146 |
DuPont Elvaloy® 1609 AC Ethylene and 9% Methyl Acrylate Copolymer Elvaloy® 1609 AC is intended for film coextrusion and injection molding. It can be recommended in film applications where softness, flexibility and excellent sealing properties are needed.Elvaloy®.. |
|||
Melting Point | 101 °C | 214 °F | Upon Melting via DSC/ASTM D3418 |
DuPont Nucrel® 903 Ethylene-Methacrylic Acid Copolymer Resin for Blown and Cast Film 9 wt% Methacrylic Acid.Nucrel® 0903 is an ethylene-methacrylic acid copolymer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process pol.. |
|||
Melting Point | 101 °C | 214 °F | DSC; ASTM D3418 |
DuPont™ Surlyn® 1652SB Zinc Ionomer Resin for Blown/Cast Film and Extrusion Coating Surlyn® 1652SB is an ionomer resin available for use in blown/cast film and extrusion coating operations. It can be used in both extrusion and coextrusion equipment designed to process polyethylen.. |
|||
Melting Point | 101 °C | 214 °F | Upon Melting via DSC/ASTM D3418 |
DuPont Elvax® 3128 Ethylene-Vinyl Acetate Copolymer Resin for Blown Film
(discontinued **) 8.9 wt% Vinyl Acetate.Elvax® 3128 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resin.. |
|||
Melting Point | 101 °C | 214 °F | Upon Melting via DSC/ASTM D3418 |
DuPont Nucrel® 0903B Ethylene-Methacrylic Acid Copolymer Resin for Blown and Cast Film
(discontinued **) 9 wt% Methacrylic Acid.Nucrel® 0903B is an ethylene-methacrylic acid copolymer resin available for use in blown and cast film extrusion and coextrusion processes designed to process polyethylene re.. |