Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melting Point = 200 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 110 - 200 °C
230 - 392 °F
Average value: 151 °C Grade Count:29
Overview of materials for Thermoplastic Polyurethane, Elastomer, Ether Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Ether Grade". Each property range of values reported is minimum a..
Melting Point 196 - 200 °C
385 - 392 °F
Average value: 197 °C Grade Count:5
Overview of materials for Nylon 6/69
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6/69". Each property range of values reported is minimum and maximum values of appropriate MatWeb ..
Melting Point 137 - 200 °C
279 - 392 °F
Huntsman IROGRAN® A 85 H 4508 TPU-Polyester
Introduction: IROGRAN A 85 H 4508 is a thermoplastic polyester- polyurethane for injection molding applications. Additional characteristics of the product are excellent mechanical properties and hig..
Melting Point 170 - 200 °C
338 - 392 °F
Huntsman/TMA
Huntsman IROGRAN® A 95 E 4813 Polyester-Based TPU-High Performance Grade
Introduction: IROGRAN A 95 R 4813 is a thermoplastic polyester- polyurethane for injection moulding applications. Additional characteristics of the product are very short cycle times and high dimens..
Melting Point 190 - 200 °C
374 - 392 °F
Huntsman/TMA
Huntsman IROGRAN® A 95 E 4861 Polyester-Based TPU-Injection Extrusion Grade
Introduction: IROGRAN A95 4861 is a high performance polyester based thermoplastic polyurethane intended for extrusion applications. IROGRAN A95E 4861 is part of the HUNTSMAN technical extrusion pro..
Melting Point 190 - 200 °C
374 - 392 °F
Huntsman/TMA
Huntsman IROGRAN® A 98 E 4735 Polyester-Based TPU-Injection Extrusion Grade
High Hydrolysis resistance and good crystallinity. Suggested for extrusion.Information provided by Huntsman
Melting Point 190 - 200 °C
374 - 392 °F
Huntsman/TMA
Huntsman IROGRAN® A 98 H 4661 Polyester-Based TPU-Injection Molding Grade
Good flow and high mechanical property performance. Suggested for injection molding.Information provided by Huntsman
Melting Point 185 - 200 °C
365 - 392 °F
Huntsman/TMA
Huntsman IROGRAN® A 98 P 4535 TPU-Polyether
Excellent resistance to hydrolysis and microbial attack. Suggested for injection molding and extrusion.Information provided by Huntsman
Melting Point 183 - 200 °C
361 - 392 °F
Indium Corp. Indalloy 113 Tin-Lead Solder Alloy
Information Provided by Indium Corporation
Melting Point 150 - 200 °C
302 - 392 °F
LG Chemical SEETEC BC500 LDPE
Good Processability and Good electrical properties. Main Application: Cable insulationCAS No. 9002-88-4Information provided by LG Chemical
Melting Point 190 - 200 °C
374 - 392 °F
MQSA 111
Lubrizol Advanced Materials Pearlthane® 12H92E Thermoplastic Polyurethane Elastomer
Pearlthane® 12H92E is a special polyester-based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent processability and excellent low temperature performance..
Melting Point 190 - 200 °C
374 - 392 °F
Temperature range at which MFI = 10 g/10 min at 21.6 kg.; MQSA 111
Lubrizol Advanced Materials Pearlthane® ECO D12T85 Thermoplastic Polyurethane
Pearlthane® ECO D12T85 is a 85 Shore A, High Performance natural TPU based on Renewable Sources with ca. 46% renewable content according to ASTM D6866 for Injection Moulding applications. This na..
Melting Point 180 - 200 °C
356 - 392 °F
0.025" extruded film,
Huntsman IROGRAN® A 92 E 4860 TPU-Polyester
Introduction: IROGRAN A92E 4860 is a high performance polyester based thermoplastic polyurethane intended for extrusion and injection molding applications. IROGRAN A92E 4860 is part of the HUNTSMAN ..
Melting Point 190 - 200 °C
374 - 392 °F
Temperature range at which MFI = 10 g/10 min at 21.6 kg.; MQSA 111
Lubrizol Advanced Materials Pearlthane® ECO D12T90E Thermoplastic Polyurethane
PEARLTHANE® ECO D12T90E is a 91 Shore A, High Performance natural TPU based on Renewable Sources with ca. 37% renewable content according to ASTM D6866 for Extrusion and Blow moulding application..
Melting Point 183 - 200 °C
361 - 392 °F
Williams Advanced Alloys WS200 Solder
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys
Melting Point 104 - 200 °C
219 - 392 °F
Average value: 113 °C Grade Count:15
Overview of materials for Low Density Polyethylene (LDPE), Wire/Cable Grade
This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Wire/Cable Grade". Each property range of values reported is minimum an..
Melting Point 190 - 200 °C
374 - 392 °F
Huntsman/TMA
Huntsman IROGRAN® A 92 K 4107 TPU-High Temperature Performance
Introduction: IROGRAN A92K 4107 is a caprolactone-based thermoplastic polyurethane. The material has been developed for injection molding applications requiring exceptional performance in terms of c..
Copyright © lookpolymers.com All Rights Reserved