Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 91.0 °C | 196 °F | Internal Method |
Polimeri Europa Greenflex® ML 40 Ethylene Vinyl Acetate Copolymer - Injection Molding Greenflex ML 40 is an ethylene vinyl acetate copolymer (EVA) for injection molding of flexible items. Items produced with Greenflex ML 40 show high elasticity and flexibility.Main Applications: Gr.. |
|||
Melting Point | 91.0 °C | 196 °F | |
LyondellBasell Lupolen® V 3510 K Ethylene Vinyl Acetate, lnjection Molding Grade Injection moldingsData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Melting Point | 91.0 °C | 196 °F | |
LyondellBasell Lupolen® V 3520 K Ethylene Vinyl Acetate Films, blow moldings.Data was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Melting Point | 91.0 °C | 196 °F | By DSC; ASTM D3418 - ISO 3146 |
DuPont Elvaloy® 1224 AC Ethylene and 24% Methyl Acrylate Copolymer Elvaloy® 1224 AC is intended for extrusion, coextrusion, compounding and injection molding. Elvaloy® 1224 AC has good adhesion to various substrates (OPA, OPP, paperboard, etc.), gives excellent .. |
|||
Melting Point | 91.0 °C | 196 °F | TRN-14 |
Tipco Tipcolite® TPF 1317 - Unreinforced Phenolic Resin with Minerals having 42 mm Norton Flow with 9% Hexamine Phenolic Resin with Minerals having 42mm Norton Flow, in Powder FormApplications: Foundry & RefractoryProcessing: Castings & ShellsInformation provided by the Manufacturer, Tipco Industries Ltd.,
In.. |
|||
Melting Point | 91.0 °C | 196 °F | by DSC; ASTM D3418 |
Westlake EBAC® SP1806 17.5%, Ethylene-Methyl Acrylate Copolymer Description: Westlake EBAC® SP1806 is an ethylene butyl acrylate copolymer designed for extrusion coating and laminating. SP1806 can also be compounded as an impact modifier or used in highly fill.. |
|||
Melting Point | 91.0 °C | 196 °F | ISO 11357 |
Total EVA 1005 VN 35 Ethylene Vinyl Acetate Copolymer - Blown Film EVA 1005 VN 35 is made by a high pressure tubular process. Grade for flexible films, with high transparency and outstanding mechanical properties. Contains NO antioxidant.Information provided by T.. |
|||
Melting Point | 91.0 °C | 196 °F | ISO 11357 |
Total EVA 1005 VN 4 Ethylene Vinyl Acetate Copolymer - Blown Film EVA 1005 VN 4 is made by a high pressure tubular process. Grade for flexible films with high transparency and good mechanical properties. Contains an antioxidant.Application examples: High strengt.. |
|||
Melting Point | 91.0 °C | 196 °F | Melting point via DSC/ASTM D3418 |
DuPont Bynel® 2002 Acid-Modified Ethylene Terpolymer Adhesive Resin Bynel® Series 2000 resins are acid-modified ethylene terpolymers with medium to high acid comonomer contents. They contain a temperature stable ester that makes them functional in high-temperature .. |
|||
Melting Point | 91.0 °C | 196 °F | Freezing Point; ASTM D3418 |
DuPont™ Bynel® 21E781 Anhydride Modified Ethylene Acrylate BYNEL® Series 2100 resins are anhydride modified ethylene acrylate resins. They contain a temperature stable ester which makes them functional in high temperature coextrusions. They are available i.. |
|||
Melting Point | 91.0 °C | 196 °F | ASTM D3418, ISO 3146 |
DuPont™ Bynel® 22E780 Modified Ethylene Acrylate BYNEL® Series 2200 resins are modified ethylene acrylate resins. They contain a temperature stable ester which makes them functional in high temperature coextrusions. They are available in pellet f.. |
|||
Melting Point | 91.0 °C | 196 °F | ASTM D3418, ISO 3146 |
DuPont™ Entira® AS MK 400 Ionomer Resin Entira™ AS MK400 is an extremely hygroscopic ionomer resin that is supplied as free-flowing pellets. |
|||
Melting Point | 91.0 °C | 196 °F | DSC |
DuPont™ Surlyn® 7940 Ionomer Resin, Lithium Surlyn® 7940 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with lithium ions. The amount of MAA and ne.. |