Polymer Property : Melting Point = 189 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 189 °C
372 °F
ASTM D3418
SK Chemicals SKYPEL P128DW Productivity Grade
SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti..
Melting Point 189 - 192 °C
372 - 378 °F
Shandong Guangyin GYBHVN Polymer
Our GYBHVN products are mainly applied in fuel pipes and brake pipes of automobile and hoses of air conditioner.Information provided by Shandong Guangyin
Melting Point 189 °C
372 °F
ISO 11357
Suzhou Hipro Polymers Hiprolon® 400 MC HLS G30 Nylon, 30% glass fiber filled
Hiprolon® 400 MC HLS G30 is a specialty long chain polyamide compound reinforced with 30% chopped glass fiber for injection molding. It contains some bio-renewable resources Features: high dime..
Melting Point <= 189 °C
<= 372 °F
Peak Melting Point; ExxonMobil method
ExxonMobil Escorene™ LD 730.09 Blown Ethylene Vinyl Acetate Copolymer
Product Description: Escorene Ultra LD 730.09 is a 17.2% vinyl acetate copolymer film resin. LD 730.09 is designed to have superior strength and toughness combined with excellent optics and sealing ..
Melting Point <= 189 °C
<= 372 °F
Peak Melting Point; ExxonMobil method
ExxonMobil Escorene™ LD 730.09 Molding Ethylene Vinyl Acetate Copolymer
Product Description: Escorene Ultra LD 730.09 is a high vinyl acetate copolymer with a low melting temperature and excellent strength properties and toughness.Availability: Latin America, North Amer..
Melting Point 189 °C
372 °F
ISO 11357
Arkema Group Rilsan® PA 11 G BMNO MED Nylon 11
Rilsan® PA 11 G BMNO MED is a polyamide produced from a renewable source. This grade offers the highest quality and it is specially designed to meet the stringent requirements of the medical applic..
Melting Point 189 °C
372 °F
ASTM D3418
ALM PA 850-Nat Nylon 11 SLS Prototyping Polymer
Unfilled PA 11 formulated for easy processing. Can be run as a drop-in replacement for other commercially available PA 11 laser sintering powders. Parts produced from PA 850 exhibit outstanding mech..
Melting Point 189 °C
372 °F
BASF Ultramid® C40 LN 07 0.04 mm Blown Film Cold Air
Information provided by BASF
Melting Point 189 °C
372 °F
ASTM D3418
ALM FR 106 Nylon 11 SLS Prototyping Polymer
This flame retardant rapid prototyping material has additives in the raw material that allows it to pass aeronautic standard FAR25.853 smoke, flame, and toxicity tests. This material is ideal for Ae..
Melting Point 189 °C
372 °F
ASTM D2117
Samyang Triel® 5300 Thermoplastic Polyether Ester Elastomer
TRIEL® resins offer superior mechanical properties, elasticities, heat and chemical resistance, which allow it to be widely used for electric/electronic equipments, automotive parts and outdoor rec..
Melting Point 189 - 192 °C
372 - 378 °F
Shandong Guangyin GYBHVNP Polymer
Our GYBHVNP products are mainly applied in fuel pipes and brake pipes of automobile and hoses of air conditioner.Information provided by Shandong Guangyin