Polymer Property : Melting Point = 122 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 30.0 - 50.0 °C
86.0 - 122 °F
BASF Diisopropanolamine S
Formula: C6H15NO2CAS: 110-97-4Description: Diisopropanolamine S is a colorless to yellow solid or melt with an amine-like odor. It is fully soluble in water.Synonyms: DIPA, 1,1’-Iminobis[2-propano..
Melting Point 46.0 - 50.0 °C
115 - 122 °F
BASF Hydroxypivalic Acid Neopentylglycolester (HPN
Formula: C10H20O4CAS: 1115-20-4Description: Hydroxypivalic Acid Neopentylglycolester (HPN) is a colorless, odorless solid.Synonyms: Neopentyl glycol monohydroxypivalate, Hydroxyneopentyl hydroxypiva..
Melting Point 46.0 - 50.0 °C
115 - 122 °F
BASF Hydroxypivalic Acid Neopentylglycolester Molten (HPN)
Formula: C10H20O4CAS: 1115-20-4Description: Hydroxypivalic Acid Neopentylglycolester Molten (HPN) is a colorless, odorless molten solid. Synonyms: Neopentyl glycol monohydroxypivalate, Hydroxyneopen..
Melting Point 30.0 - 50.0 °C
86.0 - 122 °F
BASF Diisopropanolamine
Formula: C6H15NO2CAS: 110-97-4Description: Diisopropanolamine is a colorless to yellow solid or melt with an amine-like odor. It is fully soluble in water.Synonyms: DIPA, 1,1’-Iminobis[2-propanol]..