Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | -49.0 °C | -56.2 °F | Freezing Point |
LG Chemical DINP Plasticizer Features: LG DINP is used cable and tarpaulin because it can reduce gas generation during operation due to low volatile compared to DOP.Application: Synthetic leather, sheet, power cableInformation .. |
|||
Melting Point | -49.0 °C | -56.2 °F | |
BASF 4-Chlorbutyryl Chloride Formula: C4H6Cl2OCAS: 4635-59-0Description: 4-Chlorobutyryl chloride is a colorless to yellowish liquid with a pungent odor. It hydrolyses in the presence of water.Synonyms: 4-Chlorobutanoic acid ch.. |
|||
Melting Point | -49.0 °C | -56.2 °F | |
BASF Propylencarbonate S Formula: C4H6O3CAS: 108-32-7Description: Propylencarbonate is a colorless to yellowish liquid, with a fruity odor. It is soluble in water and with many organic solvents.Synonyms: PC, Propylene carb.. |