Thermal Properties Metric English Comments
Melting Point -49.0 °C
-56.2 °F
Freezing Point
LG Chemical DINP Plasticizer
Features: LG DINP is used cable and tarpaulin because it can reduce gas generation during operation due to low volatile compared to DOP.Application: Synthetic leather, sheet, power cableInformation ..
Melting Point -49.0 °C
-56.2 °F
BASF 4-Chlorbutyryl Chloride
Formula: C4H6Cl2OCAS: 4635-59-0Description: 4-Chlorobutyryl chloride is a colorless to yellowish liquid with a pungent odor. It hydrolyses in the presence of water.Synonyms: 4-Chlorobutanoic acid ch..
Melting Point -49.0 °C
-56.2 °F
BASF Propylencarbonate S
Formula: C4H6O3CAS: 108-32-7Description: Propylencarbonate is a colorless to yellowish liquid, with a fruity odor. It is soluble in water and with many organic solvents.Synonyms: PC, Propylene carb..