Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | -38.5 °C | -37.3 °F | |
BASF 1-(2-Hydroxyethyl)piperazine Formula: C6H14N2OCAS: 103-76-4Description: 1-(2-Hydroxyethyl)piperazine is a colorless to yellowish liquid with an amine-like odor. It is miscible in water.Synonyms: 1-Amino-2-propanol, Monoisoprop.. |