Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | -33.0 °C | -27.4 °F | Freezing Point |
LG Chemical LGflex TINTM Plasticizer Features: New plasticizer is required high heat-resistance and weatherability because it is strengthen of UL standard. LGflex TINTM is excellent ins higher heat-resistance and weatherability than co.. |
|||
Melting Point | -33.0 °C | -27.4 °F | 50 vol % Aqueous Solution; ASTM D1177 |
ChevronTexaco Texcool® P 200 In service Texaco Texcool P 200 provides:Silicate freeExcellent heat transfer propertiesSuperior corrosion protection for brass, copper, solder, steel and cast ironNitrite-free, amine-freeMixes read.. |