Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | -144 °C | -227 °F | |
LG Chemical 1.3-Butadiene Physical Properties: Colorless, Slightly Sweet taste, Narcotic gas, Easy polymerization and addition reactionStructure & Characteristics: CH2=CH-CH=CH2. Unsaturated fatty acid hydrocarbon. Has a cha.. |
|||
Melting Point | -144 °C | -227 °F | |
Shandong Dongyue Shenzhou New Material Co Vinylidene Fluoride (VDF) Conformable with: Q/DYS 007-2007VDF is a kind of colorless gas under normal temperature and pressure, nontoxic, flammable, with little ether odor. It has the common gender of alkene, and can be pol.. |