Thermal Properties | Metric | English | Comments |
---|---|---|---|
Ring & Ball Softening Point | 76.0 - 220 °C | 169 - 428 °F | Average value: 113 °C Grade Count:15 |
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate; Molded/Extruded". Each property range of values reported is minimum and maximum .. |
|||
Ring & Ball Softening Point | 76.0 - 183 °C | 169 - 361 °F | Average value: 111 °C Grade Count:17 |
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade". Each property range of values reported .. |
|||
Ring & Ball Softening Point | 76.0 °C | 169 °F | ASTM E28 |
Arkema Group EVATANE® 28-800 Copolymer Ethylene - Vinyl Acetate EVATANE® 28-800 is a random copolymer of Ethylene and Vinyl Acetate made by high-pressure radicalar polymerisation process. EVATANE® 28-800 is stabilized with antioxidants. The High Vinyl Acetate .. |