Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 88.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
49.0 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Cycolac® HMG47MD ABS
General purpose, injection molding ABS for medical applications. Biocompatible (ISO10993). FDA compliant. Gamma & EtO sterilizable.
CTE, linear, Parallel to Flow 88.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
49.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycolac® MG38 ABS
Very high impact ABS. Toughness/rigidity. Good fatigue resistance.
CTE, linear, Parallel to Flow 88.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
49.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycolac® MG38 ABS (Asia Pacific)
Very high impact ABS. Toughness/rigidity. Good fatigue resistance.
CTE, linear, Parallel to Flow 88.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
49.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycolac® MG38 ABS (Europe-Africa-Middle East)
Very high impact ABS. Toughness/rigidity. Good fatigue resistance.
CTE, linear, Parallel to Flow 88.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
49.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycolac® MG38F ABS
Very high impact ABS. Toughness/rigidity. FDA compliant.
CTE, linear, Parallel to Flow 88.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
49.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycolac® MG38F ABS (Asia Pacific)
Very high impact ABS. Toughness/rigidity. FDA compliant.
CTE, linear, Parallel to Flow 88.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
49.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycolac® MG38N ABS
Very high impact ABS. Toughness/rigidity. Good fatigue resistance. NSF Standard 61 certified in limited colors (restrictions may apply)>
CTE, linear, Parallel to Flow 88.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
49.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycolac® MG38N ABS (Asia Pacific)
Very high impact ABS. Toughness/rigidity. Good fatigue resistance. NSF Standard 61 certified in limited colors (restrictions may apply)>
CTE, linear, Parallel to Flow 88.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
49.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycolac® MG47 ABS
Multi-purpose, injection molding ABS providing a favorable balance of engineering properties.
CTE, linear, Parallel to Flow 88.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
49.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycolac® MG47 ABS (Asia Pacific)
Multi-purpose, injection molding ABS providing a favorable balance of engineering properties.
CTE, linear, Parallel to Flow 88.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
49.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycolac® MG47 ABS (Europe-Africa-Middle East)
Multi-purpose, injection molding ABS providing a favorable balance of engineering properties.
CTE, linear, Parallel to Flow 88.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
49.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycolac® MG47F ABS
Multi-purpose, injection molding ABS providing a favorable balance of engineering properties. FDA compliant.
CTE, linear, Parallel to Flow 88.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
49.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycolac® MG47F ABS (Asia Pacific)
Multi-purpose, injection molding ABS providing a favorable balance of engineering properties. FDA compliant.
CTE, linear, Parallel to Flow 88.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
49.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycolac® MG47F ABS (Europe-Africa-Middle East)
Multi-purpose, injection molding ABS providing a favorable balance of engineering properties. FDA compliant.
CTE, linear, Parallel to Flow 88.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
49.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycolac® MG47N ABS
Multi-purpose, injection molding ABS providing a favorable balance of engineering properties. NSF Standard Multi-purpose, injection molding ABS providing a favorable balance of engineering properti..
CTE, linear, Parallel to Flow 88.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
49.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycolac® MG47N ABS (Asia Pacific)
Multi-purpose, injection molding ABS providing a favorable balance of engineering properties. NSF Standard Multi-purpose, injection molding ABS providing a favorable balance of engineering properti..
CTE, linear, Parallel to Flow 88.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
49.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycolac® MG94 ABS (Asia Pacific)
Superior flow, injection molding ABS. Good impact. For thin-wall applications.
CTE, linear, Parallel to Flow 88.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
49.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycolac® MGABS01 ABS
Injection molding ABS. High impact, high gloss, good flow.
CTE, linear, Parallel to Flow 88.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
49.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycolac® MGABS02 ABS
General purpose ABS. Excellent flow/impact.
CTE, linear, Parallel to Flow 88.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
49.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP STAT-KON SE003 PA 12
LNP* STAT-KON* SE003 is a compound based on Nylon 12 resin containing 15% Carbon Fiber. Added feature of this material is: Electrically Conductive.
CTE, linear, Parallel to Flow 88.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
49.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP STAT-KON SE003 PA 12 (Asia Pacific)
LNP* Stat-kon* SE003 is a compound based on Nylon 12 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.
CTE, linear, Parallel to Flow 88.2 µm/m-°C
49.0 µin/in-°F
ASTM D696
Techmer ES HiFill® HDPE TM20 20% Talc Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Talc Filler, 20% Filler by WeightInformation provided by TP Composites, Inc.
CTE, linear, Parallel to Flow 88.2 µm/m-°C
49.0 µin/in-°F
ASTM D696
Techmer ES HiFill® HDPE TM20 UV BK 20% Talc Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Talc Filler, 20% Filler by WeightAdditive: UV StabilizerFeatures: Good UV ResistanceAppearance: BlackInformation provided by TP Composi..
CTE, linear, Parallel to Flow 88.2 µm/m-°C
49.0 µin/in-°F
ASTM D696
Techmer ES HiFill® HDPE TM25 25% Talc Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Talc Filler, 25% Filler by WeightInformation provided by TP Composites, Inc.
CTE, linear, Parallel to Flow 88.2 µm/m-°C
49.0 µin/in-°F
Length
Saint-Gobain Rulon® 142 Grade Bearing/Seal PTFE
Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of..
CTE, linear, Parallel to Flow 88.2 µm/m-°C

@Temperature 20.0 °C
49.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
PlastxWorld CEVIAN®-V 320 ABS
High Impact ABSThese are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc.