Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 15.8 µm/m-°C @Temperature 23.0 - 80.0 °C |
8.78 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP D452 PC COPOLYMER (Asia Pacific) LNP* Thermocomp* D452 (or EXTC8202) is a compound based on SABIC unique Polycarbonate copolymer resin containing Glass Fiber, Flame Retardant. Added features of this material include: High modulus, .. |