Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 68.0 µm/m-°C | 37.8 µin/in-°F | ASTM D696 |
PolyOne Geon™ Vinyl Rigid Extrusion 84110 Polyvinyl Chloride, Rigid (PVC, Rigid) Note: NSF listings are obtained on specific colors. Contact PolyOne for the latest listing of approved colors for this product. Note: The Cell Classification was determined using the notched Izod te.. |
|||
CTE, linear, Parallel to Flow | 68.0 µm/m-°C | 37.8 µin/in-°F | ASTM D696 |
PolyOne Geon™ Vinyl Rigid Extrusion 87775 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
CTE, linear, Parallel to Flow | 68.0 µm/m-°C | 37.8 µin/in-°F | ASTM D696 |
PolyOne LubriOne™ PC-000/05T-2S Polycarbonate (PC) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
CTE, linear, Parallel to Flow | 68.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® 905AU PC (Asia Pacific) LEXAN resin grade 905AU is a flame retardant polycarbonate featuring non brominated and non chlorinated FR systems, with good flow, and good UV stability. It is available in all colors, intended to .. |
|||
CTE, linear, Parallel to Flow | 68.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® FXD9945A PC UV stabilzed Visualfx FR PC with non-brominated and non-chlorinated flame retardant systems. It is available Only in white diffused effect(WH8B111X) meeting UL-94 V0 at 2mm for thin wall application.. |
|||
CTE, linear, Parallel to Flow | 68.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® LUX9612G PC (Europe-Africa-Middle East) Lexan LUX9612G (EXRL0945) is a UV stabilized high viscosity, flame retardant polycarbonate featuring non brominated and non chlorinated FR system with diffusion effect and thin wall FR performance p.. |
|||
CTE, linear, Parallel to Flow | 68.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® LUX9616 PC (Asia Pacific) Lexan LUX9616 is a flame retardant polycarbonate featuring non brominated and non chlorinated FR system with diffusion effective and thin wall FR performance. It intended to meet WEEE/RoHS requireme.. |
|||
CTE, linear, Parallel to Flow | 68.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
37.8 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP COLORCOMP D1000 PC (Europe-Africa-Middle East) LNP* COLORCOMP* D1000 is a compound based on Polycarbonate resin containing Unfilled Custom Color |
|||
CTE, linear, Parallel to Flow | 68.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
37.8 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Lubricomp DBL14 PC (Europe-Africa-Middle East) Internally lubricated Polycarbonate compound, comtaining Glass Bead and PTFEThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
CTE, linear, Parallel to Flow | 68.0 µm/m-°C @Temperature 20.0 °C |
37.8 µin/in-°F @Temperature 68.0 °F |
|
Eastman Eastalloy DA003 PC+PCTG Copolyester/Polycarbonate
(discontinued **) ISO data as provided by the manufacturer, Eastman Chemical |
|||
CTE, linear, Parallel to Flow | 68.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® EXRL2032 PC (Asia Pacific) Lexan EXRL2032 is a flame retardant transparent polycarbonate featuring non brominated and non chlorinated FR system with good flow and thin wall FR performance. It intended to meet WEEE/RoHS requir.. |
|||
CTE, linear, Parallel to Flow | 68.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® LUX9612 PC (Asia Pacific) Lexan LUX9612 is a flame retardant polycarbonate featuring non brominated and non chlorinated FR system with diffusion effective and thin wall FR performance. It intended to meet WEEE/RoHS requireme.. |
|||
CTE, linear, Parallel to Flow | 68.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® LUX9616G PC (Europe-Africa-Middle East) Lexan LUX9616G (EXRL0945) is a UV stabilized high viscosity, flame retardant polycarbonate featuring non brominated and non chlorinated FR system with diffusion effect and thin wall FR performance p.. |
|||
CTE, linear, Parallel to Flow | 68.0 µm/m-°C @Temperature 20.0 °C |
37.8 µin/in-°F @Temperature 68.0 °F |
|
Ineos ABS Lustran® SAN 51 Key Features:UnfilledSuitable processing methods:Injection molding |
|||
CTE, linear, Parallel to Flow | 68.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
37.8 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP WP004 PBT LNP* LUBRICOMP* WP004 is a compound based on PBT resin containing 20% PTFE/Silicone. Added feature of this grade is: Wear Resistant. |
|||
CTE, linear, Parallel to Flow | 68.0 µm/m-°C @Temperature -40.0 - 82.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 180 °F |
ASTM D696 |
Styron CALIBREâ„¢ 200-14 Polycarbonate Resin Overview: CALIBREâ„¢ 200-14 polycarbonate resin is a natural, FDA compliant, 14 melt flow rate general purpose polycarbonate resin with no mold release or UV stabilizer.Govt. and Industry Standar.. |
|||
CTE, linear, Parallel to Flow | 68.0 µm/m-°C @Temperature -40.0 - 82.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 180 °F |
ASTM D696 |
Styron CALIBREâ„¢ 201-22 Polycarbonate Resin Overview: CALIBREâ„¢ 201-22 polycarbonate resins are produced in compliance with the US Food and Drug Administration (FDA) and EU food contact regulations. They provide excellent impact resistanc.. |
|||
CTE, linear, Parallel to Flow | 68.0 µm/m-°C @Temperature -40.0 - 82.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 180 °F |
ASTM D696 |
Styron CALIBREâ„¢ 203-22 Polycarbonate Resin Overview: CALIBREâ„¢ 200-22 polycarbonate resins are produced in compliance with the US Food and Drug Administration (FDA) and EU food contact regulations. They provide excellent impact resistanc.. |
|||
CTE, linear, Parallel to Flow | 68.0 µm/m-°C @Temperature -40.0 - 82.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 180 °F |
ISO 11359-2 |
Styron CALIBREâ„¢ 2061-6 Polycarbonate Resin Overview: CALIBREâ„¢ 2061-6 resin is suitable for steam and ethylene oxide sterilization required by the health care industry. CALIBRE 2061-6 provides excellent heat resistance, impact strength, .. |
|||
CTE, linear, Parallel to Flow | 68.0 µm/m-°C @Temperature -40.0 - 82.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 180 °F |
ASTM D696 |
Styron CALIBREâ„¢ 301-6 Polycarbonate Resin Overview: CALIBREâ„¢ 300-6 polycarbonate resins offer exceptional impact resistance, heat distortion resistance and optical clarity as well as high melt strength for blow molding and sheet applic.. |
|||
CTE, linear, Parallel to Flow | 68.0 µm/m-°C @Temperature -40.0 - 82.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 180 °F |
ASTM D696 |
Styron CALIBREâ„¢ 301V-6 Polycarbonate Resin Overview: CALIBREâ„¢ 301V-6 Polycarbonate resins offer exceptional impact resistance and heat distortion resistance, and meets UL94 V-2 rating. CALIBRE 301V-6 contains a mold release agent and is.. |
|||
CTE, linear, Parallel to Flow | 68.0 µm/m-°C @Temperature -40.0 - 82.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 180 °F |
ASTM D696 |
Styron CALIBREâ„¢ 5101-8 Polycarbonate Resin Overview: CALIBREâ„¢ 5101 Polycarbonate resins 10% glass-reinforced and provides increased modulus and improved heat distortion resistance with minimal shrinkage. This resin offers outstanding UL.. |
|||
CTE, linear, Parallel to Flow | 68.0 µm/m-°C @Temperature -40.0 - 82.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 180 °F |
ASTM D696 |
Styron CALIBREâ„¢ MEGARAD 2081-15 Polycarbonate Resin Overview: CALIBREâ„¢ MEGARAD 2081-15 Polycarbonate resin provides end-users of radiation sterilized medical devices a color closer to the water-clear look of the natural resin. When exposed to hi.. |
|||
CTE, linear, Parallel to Flow | 68.0 µm/m-°C @Temperature -40.0 - 82.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 180 °F |
ASTM D696 |
Styron CALIBREâ„¢ 200-23 Polycarbonate Resin Overview: CALIBREâ„¢ 200-23 polycarbonate resins are produced in compliance with the US Food and Drug Administration (FDA) and EU food contact regulations. They provide excellent impact resistanc.. |
|||
CTE, linear, Parallel to Flow | 68.0 µm/m-°C @Temperature -40.0 - 82.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 180 °F |
ASTM D696 |
Styron CALIBREâ„¢ 300-6 Polycarbonate Resin Overview: CALIBREâ„¢ 300-6 polycarbonate resin offer exceptional impact resistance, heat distortion resistance, and optical clarity as high melt strength for blow molding and sheet applications. .. |
|||
CTE, linear, Parallel to Flow | 68.0 µm/m-°C @Temperature -40.0 - 82.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 180 °F |
ASTM D696 |
Styron CALIBREâ„¢ 302-6 Polycarbonate Resin Overview: CALIBREâ„¢ 300-6 Polycarbonate resins offer exceptional impact resistance, heat distortion resistance, and optical clarity as well as high melt strength for blow molding and sheet appli.. |
|||
CTE, linear, Parallel to Flow | 68.0 µm/m-°C | 37.8 µin/in-°F | ASTM D696 |
Styron CALIBREâ„¢ 302V-6 LD Polycarbonate Resin Overview: CALIBREâ„¢ 302V-6 LD HC18010009 Polycarbonate is an opalescent white extrusion-grade resin containing a proprietary light diffusion package that offers an excellent combination of light.. |
|||
CTE, linear, Parallel to Flow | 68.0 µm/m-°C @Temperature -40.0 - 82.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 180 °F |
ASTM D696 |
Styron CALIBREâ„¢ 302V-6 Polycarbonate Resin Overview: CALIBREâ„¢ 302V-6 Polycarbonate resins offer exceptional impact resistance, heat distortion resistance and optical clarity (for tinted/transparent colors), and is available in both tint.. |
|||
CTE, linear, Parallel to Flow | 68.0 µm/m-°C | 37.8 µin/in-°F | ISO 11359-1/-2 |
Covestro Bayblend® FR 3006 Polycarbonate + ABS, Flame Retardant Grade Injection molding gradehigh heat resistanceVicat/B 120 = 110 °Ceasy flowUL-listing 94 V-1 at 1.5 mm and V-0 at 2.0 mmPreprocessingMax. Water content |
|||
CTE, linear, Parallel to Flow | 68.0 µm/m-°C | 37.8 µin/in-°F | ISO 11359-1/-2 |
Covestro Bayblend® KU 2-1514 BBS073* Polycarbonate + ABS, Flame Retardant Grade Developmental productHigh heat resistant injection molding gradeimproved chemical resistance and stress cracking behavior compared to KU 2-1514ball indentation temperature = 125 °CVicat/B 120 tempe.. |