Polymer Property : CTE, linear, Parallel to Flow = 63.3 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 114 µm/m-°C

@Temperature 20.0 °C
63.3 µin/in-°F

@Temperature 68.0 °F
Eastman Tenite 180A-28(HT) Cellulose Acetate  (discontinued **)
28% Plasticized.ISO data as provided by the manufacturer, Eastman Chemical.
CTE, linear, Parallel to Flow 114 µm/m-°C

@Temperature 23.0 - 60.0 °C
63.3 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP KA000M POM (Europe-Africa-Middle East)
LNP* LUBRICOMP* KA000M is a compound based on Acetal Copolymer resin containg Aramide and Proprietary Lubricant. Added features include Internally Lubricated.
CTE, linear, Parallel to Flow 114 µm/m-°C

@Temperature -30.0 - 30.0 °C
63.3 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP STAT-KON FD000 PE
LNP* STAT-KON* FD000 is an unfilled Polyethylene. Added feature of this grade is: Electrically Conductive.