Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 12.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
6.67 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP 9X98026 PA 46 (Europe-Africa-Middle East) LNP* Lubricomp* 9X98026 is a compound based on PA4.6 resin containing Barium Sulfate, PTFE and Carbon Fiber |
|||
CTE, linear, Parallel to Flow | 12.0 µm/m-°C @Temperature 20.0 °C |
6.67 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
Mitsubishi Xantar® SF 2220 Polycarbonate-20% Glass Reinforced Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
CTE, linear, Parallel to Flow | 12.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
6.67 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP STAT-KON RE004 PA 66 (Europe-Africa-Middle East) LNP* Stat-kon* RE004 is a compound based on Nylon 66 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
CTE, linear, Parallel to Flow | 12.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
6.67 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D 696 |
SABIC Innovative Plastics LNP Stat-kon TD000 LNP* Stat-kon* TD000 is a compound based on Polyurethane resin. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Parallel to Flow | 12.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
6.67 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP STAT-KON TD000 PU LNP* STAT-KON* TD000 is an unfilled compound based on Polyurethane resin. Added feature of this material is: Electrically Conductive. |
|||
CTE, linear, Parallel to Flow | 12.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
6.67 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Thermocomp PF00A PA 6 (Europe-Africa-Middle East) 50% glass fibre reinforced Polyamide 6 injection moulding resin.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
CTE, linear, Parallel to Flow | 12.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
6.67 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP QC006 PA6.10 LNP THERMOCOMP* QC006 is a compound based on Nylon 6/10 resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
CTE, linear, Parallel to Flow | 12.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
6.67 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP UX06003 PPA (Europe-Africa-Middle East) LNP* THERMOCOMP* UX06003 is a compound based on Polyphalamide resin containing Carbon Fiber. Added features include Electrically Conductive, Mold Release, Heat Stabilized. |
|||
CTE, linear, Parallel to Flow | 12.0 µm/m-°C @Temperature 20.0 °C |
6.67 µin/in-°F @Temperature 68.0 °F |
ASTM E-831 |
Sumitomo Bakelite North America EM 7302 Hardware Grade Epoxy Long fiberglass reinforced epoxy molding compound which features high strength and toughness for structural components. This compound is designed for applications requiring Mil-M-46069 certificatio.. |
|||
CTE, linear, Parallel to Flow | 12.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
6.67 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP STAT-KON DX05042 PC (Europe-Africa-Middle East) LNP* Stat-kon* DX05042 is a compound based on Polycarbonate resin containing Glass Fiber, PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive, Easy Molding. |
|||
CTE, linear, Parallel to Flow | 12.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
6.67 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Thermocomp RF00AES PA 66 (Europe-Africa-Middle East) LNP THERMOCOMP* RF00AES is a compound based on PA66 resin containing Glass Fiber, Mold Release.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
CTE, linear, Parallel to Flow | 12.0 µm/m-°C | 6.67 µin/in-°F | TMA |
Vyncolit X655RB Glass Fiber and Mineral Filled Novolac Phenolic Novolac resin based, glass fiber and mineral reinforced. Grade with superior stiffness, high dimensional stability and high wear resistance. Good chemical resistance against several fuels at elevate.. |
|||
CTE, linear, Parallel to Flow | 12.0 µm/m-°C @Temperature 23.0 - 150 °C |
6.67 µin/in-°F @Temperature 73.4 - 302 °F |
ASTM E 228 |
DuPont Performance Polymers VESPEL TP-8541 Polyimide Thermoplastic parts from filled PI (polyimide) for high mechanical properties and impact performance in high temperature environmentsInformation provided by DuPont Performance Polymers |
|||
CTE, linear, Parallel to Flow | 12.0 µm/m-°C @Temperature 55.0 - 160 °C |
6.67 µin/in-°F @Temperature 131 - 320 °F |
DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® HTN FR52G30NHF BK337 Polyphthalamide (PPA) 30% Glass Reinforced Flame Retardant Non-Halogenated PPA High Performance Polyamide with Improved Flow Zytel HTNFR52G30NHF BK337 is a 30% glass reinforced flame retardant lubricated high performance.. |
|||
CTE, linear, Parallel to Flow | 12.0 µm/m-°C | 6.67 µin/in-°F | DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® HTN FR55G50NHLW BK046 Polyphthalamide (PPA)
(Unverified Data**) 55% Glass Reinforced Flame Retardant Non-Halogenated PPA High Performance Polyamide with Low Warpage and High Stiffness Zytel HTNFR55G50NHLW BK046 is a 50% glass reinforced flame retardant high perf.. |
|||
CTE, linear, Parallel to Flow | 12.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
6.67 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Staramide BG10 PA6, 50% Glass Filled, Injection Molded BG10 is a 50% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
CTE, linear, Parallel to Flow | 12.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
6.67 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Staramide BG10H PA6, 50% Glass Filled, Injection Molded BG10 is a Heat Stabilized, 50% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
CTE, linear, Parallel to Flow | 12.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
6.67 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Staramide BG10HU PA6, 50% Glass Fiber Filled, UV and Heat Stabilized, Injection Molded Staramide BG10HU is an UV and Heat Stabilized, 50% Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
CTE, linear, Parallel to Flow | 12.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
6.67 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Staramide RF00AES PA66/6, 50% Glass Filled, Injection Molded Staramide RF00AES is a 50% Glass Fiber Reinforced Polyamide 66/Polyamide 6 Injection Molding Resin (also known as Staramide 66 C 50V S3)Information provided by Eurostar. |
|||
CTE, linear, Parallel to Flow | 12.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
6.67 µin/in-°F @Temperature 73.4 - 131 °F |
DIN 53752 |
BASF Ultraform H 4320 Q600 POM Ultraform H4320 Q600 is an extrusion POM high molecular weight grade. This grade enables high extrusion rates with thick-walled product. It also exhibits high thermal stability and a low tendency .. |
|||
CTE, linear, Parallel to Flow | 12.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
6.67 µin/in-°F @Temperature 73.4 - 131 °F |
DIN 53752 |
BASF Ultraform® N2320 006 POM Description: Is a POM, high-molecular-weight grade with somewhat increased flowability for injection molding of relatively thick-walled moldings.Information provided by BASF |
|||
CTE, linear, Parallel to Flow | 12.0 µm/m-°C @Temperature 55.0 - 160 °C |
6.67 µin/in-°F @Temperature 131 - 320 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Rynite® FR515 NC010 Polyethylene Terephthalate (PET)
(Unverified Data**) 15% Glass Reinforced Flame Retardant Polyethylene Terephthalate Rynite FR515 NC010 is a flame retardant 15% glass reinforced modified polyethylene terephthalate. Recognized by UL as UL94V-0 at 0.8mm.. |
|||
CTE, linear, Parallel to Flow | 12.0 µm/m-°C | 6.67 µin/in-°F | ASTM E831 |
Sumitomo Bakelite North America RX® 680 Fiberglass and Glass Reinforced Phenolic RX 680 is a fiberglass and glass bead filled phenolic molding compound, with good dimensional stability and good strength at elevated temperatures.Information provided by Sumitomo Bak North America,.. |
|||
CTE, linear, Parallel to Flow | 12.0 µm/m-°C | 6.67 µin/in-°F | Below Tg; ISO 11359 |
Victrex® PEEK 150FC30 Easy Flow Product Description: High performance thermoplastic material, 30% reinforced with carbon fibre / graphite / PTFE PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding, easy .. |